Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.93 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87727-0284 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples. Physical property testing was based on the Geon® 87727 Trans 0020.Information provided by PolyOne |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
3.93 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.18 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 1010 A Natural Polyamide 6 (Nylon 6) The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of .. |
|||
Izod Impact, Notched | 2.10 J/cm @Temperature 23.0 °C |
3.93 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWM206 ASA Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 2.10 J/cm @Temperature 23.0 °C |
3.93 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Asia Pacific) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Asia Pacific regio.. |
|||
Izod Impact, Notched | 2.10 J/cm @Temperature 23.0 °C |
3.93 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.18 mm, Temperature -20.0 °C |
3.93 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-BW00 Natural Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 300DA Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(discontinued **) Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Powder grades for masterbatches.Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 513LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 901 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 1450LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polyme.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 300DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Features: Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 .. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 350LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 513LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: MonofilamentsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solv.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 930LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 902 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 28.0 J/g; Heat of Fusion - ASTM D3418 28.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Izod Impact, Notched | 2.10 J/cm @Temperature 23.0 °C |
3.93 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 1.7%); ASTM-D256 |
Toyobo GLAMIDE® T-602G30 MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 2.10 J/cm @Temperature 23.0 °C |
3.93 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |