Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.910 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87549 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
1.70 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5705 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature 22.8 °C |
1.70 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature -30.0 °C |
1.70 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-G15 Modified-PPO, 15% Glass Reinforced, High Flow Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastalloy DA510 Polymer
(discontinued **) Eastalloy Polymer DA510 is a clear copolyester/polycarbonate alloy. This product has good physical properties. These include good impact strength, chemical resistance, heat resistance, dimensional s.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastalloy MA510 Polymer
(discontinued **) Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhan.. |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.70 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM-D256 |
Ineos ABS Lustran® 256/Lustran® 752 Blended ABS Resin 50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.70 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM-D256 |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature -20.0 °C |
1.70 ft-lb/in @Temperature -4.00 °F |
1/8'' notched bar; ASTM D256 |
Ineos 3560 Polypropylene Impact Copolymer This is a special high melt flow, nucleated, high impact copolymer polypropylene for injection molding applications. It offers excellent impact resistance and a high flexural modulus.ApplicationsAu.. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature -20.0 °C |
1.70 ft-lb/in @Temperature -4.00 °F |
1/8'' notched bar; ASTM D256 |
Ineos T20N-00 Polypropylene Impact Copolymer This is a special high melt flow, nucleated, high impact copolymer polypropylene for injection molding applications. It offers excellent impact resistance and a high flexural modulus.ApplicationsCo.. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature -17.8 °C |
1.70 ft-lb/in @Temperature 0.000 °F |
1/8" x 1/2" bar; ASTM-D256 (Method A) |
Ineos ABS Lustran® Guardian™ 620 ABS, Extrusion Grade Lustran® Guardian™ ABS 620 is a high modulus, HFC 134a and HCFC 22 resistant extrusion grade resin designed for refrigerator door and food liners. Lustran® ABS 620 offers good melt streng.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -20.0 °C |
1.70 ft-lb/in @Temperature -4.00 °F |
ASTM D 256 |
MRC Polymers SATRANâ„¢ 805 ABS Terpolymer, Impact Modified Information provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 6.35 mm |
1.70 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PlastxWorld CEVIAN®-V T180 ABS High Modulus ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature -18.0 °C |
1.70 ft-lb/in @Temperature -0.400 °F |
ASTM D256 |
Formosa Plastics Formolene® 6610A Impact Copolymer Polypropylene Impact Copolymer for Compounding and Injection Molded Applications Formolene® 6610A is a high impact copolymer of polypropylene designed for such injection applications as automotive compounding, l.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature 22.8 °C |
1.70 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant ABS4500 ABS, High Impact Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature 22.8 °C |
1.70 ft-lb/in @Temperature 73.0 °F |
ASTM D256A |
ExxonMobil AP3AW Polypropylene Impact Copolymer Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe.. |