Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
11.2 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0152 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Asia Pacific) Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Europe-Africa-Middle East) Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | >= 6.00 J/cm @Temperature 23.0 °C |
>= 11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 8332C (EPD60R) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 4301 PPC+PC Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | >= 6.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 11.2 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa LONOY 1600 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Izod Impact, Notched | 6.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.2 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa MAC-851 PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
3.2 mm (0.125 in) notch |
Kraton® G1650 + PP blend + Talc (12/21/67) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Izod Impact, Notched | >= 6.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 11.2 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa LONOY 2100 LT PC/PET Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature -30.0 °C |
11.2 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron PULSEâ„¢ EXT 200 PC/ABS Engineering Resin Overview: High Heat, High Impact PC/ABS resin for injection molded automotive plating and painting trim applications.Information provided by Styron |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND 7500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, good thermal and mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND PSA 8500 V0 HF Flame Retardant PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendFlame retardant class V0, chlorine and bromine free, excellent light resistance, high impact resistance, excellent processabilityInformation pro.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 0400 OPALE Polycarbonate Polycarbonate for injection or extrusionOpal, light diffusiveInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 0501 Polycarbonate Polycarbonate for injection or extrusionHigh impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 1001 Polycarbonate General purpose polycarbonateHigh impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 1060 V0 HF Flame Retardant Polycarbonate Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistanceInformation pro.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 1560 V0 HF Flame Retardant Polycarbonate Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistanceInformation pro.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 1601 Polycarbonate General purpose polycarbonateHigh melt flow rate, high impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 6.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.2 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon FR-PC V0 Polycarbonate Characteristics: self-extinguishing V0 at 1,6 mm |
|||
Izod Impact, Notched | 6.00 - 8.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.2 - 15.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon PC IX3000 Polycarbonate, High Impact Characteristics: high fluidity, high impact |
|||
Izod Impact, Notched | 6.00 - 8.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.2 - 15.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon PC UVR Polycarbonate, High Impact Characteristics: high fluidity, high impact, UV resistant |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® TR 50 Polypropylene Impact Copolymer Description: CAPILENE® TR 50 is a medium melt flow rate heterophasic copolymer with very high impact strength, even at low temperature, designed for injection molding. This grade combines good pr.. |