Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS (Europe-Africa-Middle East) High stiffness PC/ABS blend offering high impact, high heat, low CTE, good surface quality and excellent extrusion and thermoforming characteristics.This data was supplied by SABIC-IP for the Europe.. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Izod Impact, Notched | >= 5.00 J/cm @Temperature 23.0 °C |
>= 9.37 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 8300G (EPYS30RE) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 5.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
9.37 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Mapal Plastics Maplon Type H Polypropylene Sheet Properties : Good resistance to low temperatures, Moderate stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printing.Applications : Stationery, Printing.. |
|||
Izod Impact, Notched | 5.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
9.37 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH960 6111 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesHigh heat resistanceChemical resistance, hydrolysis resistanceGood paint adhesionHigh flow ability,.. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 0.000 °C |
9.37 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Izod Impact, Notched | 5.00 J/cm @Thickness 3.17 mm |
9.37 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.00 J/cm @Thickness 3.17 mm |
9.37 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ISO R 180 |
Styron Pulse® A20-95 PC/ABS A medium impact strength PC/ABS blend with high heat distortion and excellent processability.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND 4500 T V0 Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, PBDE free, with halogens, high impact resistance, high thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 0.000 °C |
9.37 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTABLEND 4501 V0/D Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, PBDE and antimony free, with halogens, high impact resistance, very high thermal resistance, high gloss, good processabilityInformation provided by Cossa Poli.. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND 6500 F Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blendHigh melt flow rate, good thermal resistance, good impact resistance, excellent processability, good surface appearanceInformation provided by .. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND 6500 Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blendHigh thermal resistance, high impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 0.000 °C |
9.37 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTABLEND 8500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, good thermal and mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l.. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 0.000 °C |
9.37 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND PSA 7400 HF PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendHigh impact resistance, high gloss, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 0.000 °C |
9.37 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND PSA 8500 V0 Flame Retardant PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendFlame retardant class V0, excellent light resistance, high impact resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 0.000 °C |
9.37 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTACARB 0400 OPALE Polycarbonate Polycarbonate for injection or extrusionOpal, light diffusiveInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 0.000 °C |
9.37 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTACARB 0501 Polycarbonate Polycarbonate for injection or extrusionHigh impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 0.000 °C |
9.37 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTACARB 1001 Polycarbonate General purpose polycarbonateHigh impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 0.000 °C |
9.37 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTACARB 1560 V0 Flame Retardant Polycarbonate Flame retardant class V0, antimony and PBDE free, opaque, high melt flow, high impact strength, high thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 0.000 °C |
9.37 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTACARB 1601 Polycarbonate General purpose polycarbonateHigh melt flow rate, high impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 2060 V0 Flame Retardant Polycarbonate Flame retardant class V0, antimony and PBDE free, opaque, high melt flow, high impact strength, high thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 2060 V0 HF Flame Retardant Polycarbonate Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistanceInformation pro.. |
|||
Izod Impact, Notched | 5.00 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
9.37 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon FR-PC V0 Polycarbonate Characteristics: self-extinguishing V0 at 1,6 mm |
|||
Izod Impact, Notched | >= 5.00 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
>= 9.37 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon PC IX3000 Polycarbonate, High Impact Characteristics: high fluidity, high impact |
|||
Izod Impact, Notched | 5.00 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
9.37 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PA 1406 PRE-ELEC PA 1406 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon fiber. In addition to a low electrical resistivity PRE-ELEC PA 1406 .. |