Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.00 J/cm @Temperature -30.0 °C |
7.49 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East) UV stabilized, non-FR PC/ABS of excellent flow and impact performanceThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 4.00 J/cm @Temperature 23.0 °C |
7.49 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Izod Impact, Notched | 4.00 J/cm @Thickness 3.17 mm |
7.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trilac® ABS-HS7500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 4.00 J/cm @Thickness 3.20 mm, Temperature -32.0 °C |
7.49 ft-lb/in @Thickness 0.126 in, Temperature -25.6 °F |
ASTM D256 |
Kingfa MAC-851 PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Izod Impact, Notched | 4.00 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
7.49 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM-D256 |
Ineos ABS Lustran® 786 ABS, Extrusion Grade Lustran® ABS 786 resin is a black, virgin extrusion grade of ABS (acrylonitrile butadiene styrene). It is designed for extruded drain, waste, and vent (DWV) pipe. Lustran® ABS 786 (901046 blac.. |
|||
Izod Impact, Notched | 4.00 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
7.50 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8006 Availability: North AmericaForms: PelletsProcessing Method: Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.00 J/cm @Temperature 23.0 °C |
7.49 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl EM6100F PPE+PS Automotive interiors. 240F HDT. High impact/good property retention after heat ageing. In blowmolding, better sandability of flash, overblow.This data was supplied by SABIC-IP for the Americas re.. |
|||
Izod Impact, Notched | >= 4.00 J/cm @Temperature 23.0 °C |
>= 7.49 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 2.4%); ASTM-D256 |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 4.00 J/cm @Thickness 3.17 mm |
7.49 ft-lb/in @Thickness 0.125 in |
|
TPI Porene® ABS-SP-100 Super High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 4.00 J/cm @Temperature 23.0 °C |
7.49 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 3.5%); ASTM-D256 |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 4.00 J/cm @Temperature 23.0 °C |
7.49 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 3008 MT Acrylonitrile Butadiene Styrene ABS with very high impact resistanceHigh impact resistance at low temperature, medium heat resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 4.00 J/cm @Temperature 23.0 °C |
7.49 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE CR 1 Acrylonitrile Butadiene Styrene ABS for chrome platingGood melt flow rate, high impact resistance at low temperature, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | >= 4.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 7.49 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epicarb PC Polycarbonate Characteristics: high fluidity, good impact |