Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.76 J/cm @Temperature -30.0 °C |
3.30 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Noble Polymers Regis™ 230106 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 3.17 mm |
3.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LG Chemical SI-610 Alphalac Polystyrene High flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include big size electric app.. |
|||
Izod Impact, Notched | 1.76 J/cm @Temperature -29.0 °C |
3.30 ft-lb/in @Temperature -20.2 °F |
3.2 mm (0.125 in) notch |
Kraton® FG1901 + PA-6,6 blend (20/80) Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.30 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa FRABS V-0 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmHigh toughnessFor extrusion moldingApplications:PlateElectric and electronic cabinetPCB boardInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
3.30 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM-D256 |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Izod Impact, Notched | 1.76 J/cm @Temperature -30.0 °C |
3.30 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Europe-Africa-Middle East) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 1.76 J/cm @Temperature -30.0 °C |
3.30 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.76 J/cm @Temperature -30.0 °C |
3.30 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 1.76 J/cm @Temperature -30.0 °C |
3.30 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
3.30 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8010 Availability: North AmericaForms: PelletsProcessing Method: Extrusion Blow Molding and Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 6.35 mm |
3.30 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 6.35 mm |
3.30 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.76 J/cm @Temperature 23.0 °C |
3.30 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl INT1000 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.76 J/cm @Temperature -30.0 °C |
3.30 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.30 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 140V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.30 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 140Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
3.30 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 300Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.30 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 340W Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 6.40 mm |
3.31 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron AN-312 Flame Retardant ABS Grade |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 3.20 mm |
3.31 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron AN-450 Flame Retardant ABS Grade Information provided by Bhansali |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 6.40 mm |
3.31 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 3.20 mm |
3.31 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron AN-450 EVM Flame Retardant ABS Grade Information provided by Bhansali |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 3.20 mm |
3.31 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron AN-450 Flame Retardant ABS Grade Information provided by Bhansali |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 6.40 mm |
3.31 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
3.30 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
0.5 x 0.125 in.; ASTM D256 |
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin STYRON™ 487 is a high-impact polystyrene with an excellent balance of flow, toughness, stiffness and heat resistance. It has excellent deep draw characteristics and is appropriate for extrusion ap.. |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 3.20 mm |
3.31 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron AN-450 EVM Flame Retardant ABS Grade Information provided by Bhansali |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 6.40 mm |
3.31 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron AN-312 Flame Retardant ABS Grade |
|||
Izod Impact, Notched | 1.76 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.30 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 300V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |