| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical LI933 Co-Extrusion ASA Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical LUMID HI2152A(W) PA6+GF15%, High Impact Feature: Injection Molding, PA6+GF15%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical TR556 MABS, Transparency, Chemical Resistance Feature: Injection Molding, Transparency, Chemical ResistanceApplication: Sound Proofing Wall, Canopy, Other Transparent SheetsCAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical.. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical TR556 MABS, Transparency, Chemical Resistance Feature: Injection Molding, Transparency, Chemical ResistanceApplication: Sound Proofing Wall, Canopy, Other Transparent SheetsCAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical.. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
| Izod Impact, Notched | >= 1.77 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 3.31 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical LUPOL HM5204 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.35 mm |
3.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Infino® GW-3130 PC, 10% Glass Filled Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 3.17 mm |
3.31 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Starex® LX-0989EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 3.17 mm |
3.31 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Starex® SR-0315 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.35 mm |
3.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Infino® GW-3130 PC, 10% Glass Filled Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 3.17 mm |
3.31 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Starex® LX-0989EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 3.17 mm |
3.31 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Starex® NH-0927 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 3.17 mm |
3.31 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Starex® SR-0315 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.35 mm |
3.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Starex® VC-0830 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.76 J/cm @Thickness 6.40 mm |
3.31 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
| Bhansali Engineering Abstron AN-312 Flame Retardant ABS Grade |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 3.20 mm |
3.31 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
| Bhansali Engineering Abstron AN450M Flame Retardant ABS Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali |
|||
| Izod Impact, Notched | 1.76 J/cm @Thickness 6.40 mm |
3.31 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
| Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.40 mm |
3.31 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
| Bhansali Engineering Abstron KU650N ABS Heat Resistant Medium/High ImpactInformation provided by Bhansali |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 3.20 mm |
3.31 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
| Bhansali Engineering Abstron KU650NH ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
| Izod Impact, Notched | 1.76 J/cm @Thickness 6.40 mm |
3.31 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
| Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
| Izod Impact, Notched | 1.76 J/cm @Thickness 3.20 mm |
3.31 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
| Bhansali Engineering Abstron AN-450 EVM Flame Retardant ABS Grade Information provided by Bhansali |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.40 mm |
3.31 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
| Bhansali Engineering Abstron IM21G ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |
|||
| Izod Impact, Notched | 1.76 J/cm @Thickness 6.40 mm |
3.31 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
| Bhansali Engineering Abstron AN-312 Flame Retardant ABS Grade |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 3.20 mm |
3.31 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
| Bhansali Engineering Abstron AN450M Flame Retardant ABS Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.40 mm |
3.31 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
| Bhansali Engineering Abstron IM21G ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |
|||