Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87547 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87548 AS Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent PVC profile compound, with reduced surface resistivity, resulting in unlikely attraction and adhesion of dust. Actual results on surface resistivity = 1.3x10^15.Information provided by.. |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87548 Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent PVC profile compound, with inherent water clear optical characteristics.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87554 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87555 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87556 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0659 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0660 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0678 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy FXTW26SK ASA Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXD104R PC (Europe-Africa-Middle East) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regi.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer (Asia Pacific) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer (Europe-Africa-Middle East) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa.. |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Shell Carilon® DP R1130 Polyketone, 30% Glass Fiber Reinforced
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1130 is a 30 percent glass fiber reinforced compound based on a developmental e.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Asia Pacific) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Asia Pacific region... |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Europe-Africa-Middle East) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -20.0 °C |
2.62 ft-lb/in @Temperature -4.00 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East) XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.17 mm |
2.62 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LG Chemical SG-910 Alphalac Polystyrene
(Unverified Data**) High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliances |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LATAN 3E71 Polyoxymethylene Copolymer (POM) with Elastomer
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LI-943 ASA Resin
(discontinued **) Heat resistance, Excellent weather resistance, Well balanced mechanical properties, Superior chemical resistance, Good thermal aging stability, Good moldability and processability, Applications incl.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -40.0 °C |
2.62 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 2.0%); ASTM-D256 |
Toyobo GLAMIDE® T-403 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 1.75%); ASTM-D256 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -40.0 °C |
2.62 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -40.0 °C |
2.62 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -40.0 °C |
2.62 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 0.8%); ASTM-D256 |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |