Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar GN002 Copolyester, Natural
(discontinued **) Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar GN005 Copolyester, Natural
(discontinued **) Eastar GN005 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN005 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.89 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa HR-528 Modified ABS Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature -20.0 °C |
1.90 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Ineos N00N-00 Polypropylene Impact Copolymer Grade N00N-00 is a fractional melt flow rate, high impact copolymer polypropylene specifically designed for non-pressure structured wall pipe but can also be used in other extrusion applications req.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature -20.0 °C |
1.90 ft-lb/in @Temperature -4.00 °F |
1/8" (3mm) notched bar; ASTM D256 |
Ineos N10N-00 Polypropylene Impact Copolymer Grade N10N-00 is a nucleated polypropylene impact copolymer with an excellent balance of stiffness and impact resistance for injection molding applications and compounding products used in Lawn and .. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF30 IM BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF33 IM L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File N.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF33 IM2 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF33 IM3 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF40 IM HS UV RD 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS GN005 Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: GreenInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS NAT Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS/PA 1700 B1 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -28.9 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -20.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/ABS 720 BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES HiFill® PA6 LGF30 HS L 12mm 30% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedIn.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS SL2 Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS TL2 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 92RK Availability: North AmericaForms: PelletsFeatures: General PurposeProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS LE WT Availability: North AmericaForms: PelletsFeatures: Low Extractables and Medium Impact ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Drystar 0113 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Drystar 0601 Copolyester, Injection Molded This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar MN210 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates.Applications/UsesMedical |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar MN211 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. MN211 contains a mold release.Application.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman GSP01 Copolyester for Film and Sheet Extrusion Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8008 Availability: North AmericaForms: PelletsFeatures: General Purpose Appearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS/PA 1700 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS SLX2 MB Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS TL10 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS X MB Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |