Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.500 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
0.937 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ISO 180/4A |
Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
0.937 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -20.0 °C |
0.937 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LASTIROL TR-V0 Polystyrene (PS) (UL94 V-0)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Izod Impact, Notched | >= 0.500 J/cm @Temperature -20.0 °C |
>= 0.937 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 8300G (EPYS30RE) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 3.20 mm, Temperature -20.0 °C |
0.937 ft-lb/in @Thickness 0.126 in, Temperature -4.00 °F |
ASTM D256 |
Mapal Plastics Maplon CFA-HK Polypropylene Sheet Applications: For use with electrical insulation products. For use when flame retardant and static dissipative properties are required. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 23.0 °C |
0.937 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 23.0 °C |
0.937 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 6.35 mm |
0.937 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 6.35 mm |
0.937 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -40.0 °C |
0.937 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 23.0 °C |
0.937 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 0.000 °C |
0.937 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 0417 GIF Acrylonitrile Butadiene Styrene, 17% Glass Filled ABS with 17% glass fiber reinforcementGood thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 23.0 °C |
0.937 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP 0540 GFC V0 Flame Retardant Polypropylene, 20% Glass Filled PP with 20% chemically coupled glass fiberFlame retardant class V0, excellent mechanical characteristics, excellent heat resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 0.000 °C |
0.937 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP 1006 V2 K Flame Retardant Polypropylene PP copolymerFlame retardant class V2, PBDE and antimony trioxide free, no blooming, low smoke emission, good physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -20.0 °C |
0.937 ft-lb/in @Temperature -4.00 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 0540 GFC Polypropylene, 20% Glass Filled PP homopolymer 20% chemically coupled glass fiber reinforcedInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 0.000 °C |
0.937 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 0560 GF Polypropylene, 30% Glass Filled PP homopolymer 30% glass fiber reinforcedGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 0.000 °C |
0.937 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP KUR 0550 V0 HF Flame Retardant Polypropylene PP copolymer elastomer modifiedFlame retardant class V0, halogen free, high impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 0.000 °C |
0.937 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTASTIR HG 0808 Polystyrene High gloss polystyreneHigh impact resistance, good physical and mechanical characteristics, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
0.937 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac R ABS 10% GF Acrylonitrile Butadiene Styrene, 10% Glass Fiber Characteristics: 10% glass fibre filled |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
0.937 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac R ABS 17% GF ABS, 17% Glass Fiber Characteristics: 17% glass fibre filled |
|||
Izod Impact, Notched | 0.500 - 0.600 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.937 - 1.12 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -20.0 °C |
0.937 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Braskem CP 241 Injection Molding Polypropylene Description: CP 241 is a high melt flow rate heterophasic copolymer used for general purposes. This product offers excellent processability, easy mould filling, productivity as well as good stiffnes.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -20.0 °C |
0.937 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Carmel Olefins CAPILENE® HT 75 A Polypropylene Impact Copolymer Description: CAPILENE® HT 75 A is a nucleated and antistatic high flow impact copolymer for injection molding. It is characterized by improved stiffness, medium impact resistance and good organol.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -20.0 °C |
0.937 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Carmel Olefins CAPILENE® SU 75 AV Polypropylene Impact Copolymer Description: CAPILENE® SU 75 AV is a high melt flow rate, controlled rheology impact copolymer for injection molding. CAPILENE® SU 75 AV is nucleated with antistatic additive. It offers outstand.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 23.0 °C |
0.937 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Braskem Symbios 4102 Polypropylene Terpolymer Braskem Symbios 4102 is a medium melt flow rate terpolymer with a heat seal temperature below 120ºC on its treated face. It is designed for use as a heat sealing layer on bioriented films (BOPP) an.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -20.0 °C |
0.937 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Carmel Olefins CAPILENE® SR 50 Polypropylene Impact Copolymer Description: CAPILENE® SR 50 is a medium melt flow rate impact copolymer for injection molding applications. This grade offers good balance of stiffness, impact strength and processability.Applic.. |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
0.937 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PA 1406 PRE-ELEC PA 1406 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon fiber. In addition to a low electrical resistivity PRE-ELEC PA 1406 .. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -40.0 °C |
0.937 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 23.0 °C |
0.937 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® V9235 PET (Europe-Africa-Middle East) Valox heat stabilized, 15% Glass filled grade with mold release based on recycle PET. This grade is typically applied for business Machines applicationsThis data was supplied by SABIC-IP for the Eu.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -30.0 °C |
0.937 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® V9235 PET (Europe-Africa-Middle East) Valox heat stabilized, 15% Glass filled grade with mold release based on recycle PET. This grade is typically applied for business Machines applicationsThis data was supplied by SABIC-IP for the Eu.. |