Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.300 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
0.562 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PC/ABS 1420 PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR.. |
|||
Izod Impact, Notched | 0.300 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
0.562 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PS 1328 PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX2415 PC Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -40.0 °C |
0.562 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -40.0 °C |
0.562 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -40.0 °C |
0.562 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-422VOR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP 1040 T8 V0 Flame Retardant Polypropylene Flame retardant class V0, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP 1040 V2 H Flame Retardant Polypropylene PP homopolymerFlame retardant class V2, halogen free, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H 10100 BS Polypropylene, 50% Mineral Filled PP homopolymer 50% mineral fillerExcellent surface appearance, high densityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H 1080 TG Polypropylene, 40% Mineral Filled PP homopolymer 40% mineral fillerExcellent stiffness, good dimensional stabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP HK 1280 T8 Polypropylene, 40% Mineral Filled PP homopolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP HK 2540 T8 Polypropylene, 20% Mineral Filled PP homo/copolymer 20% mineral fillerGood physical and mechanical propertiesInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -20.0 °C |
0.562 ft-lb/in @Temperature -4.00 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP KUR 0550 V0 HF Flame Retardant Polypropylene PP copolymer elastomer modifiedFlame retardant class V0, halogen free, high impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.300 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.562 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac R ABS 10% GF Acrylonitrile Butadiene Styrene, 10% Glass Fiber Characteristics: 10% glass fibre filled |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTASAN SAN 0840 GF Styrene Acrylonitrile SAN with 20% glass fiber reinforcementExcellent dimensional stability, good heat resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -20.0 °C |
0.562 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Braskem CP 145 Injection Molding Polypropylene Applications: Household; thin-walled parts; easy mould filling. Information provided by Braskem |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -20.0 °C |
0.562 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Braskem CP 204 Injection Molding Polypropylene Description: CP 204 is a high melt flow rate heterophasic copolymer with general purpose additive package. This product exhibits excellent processing performance, with good stiffness and impact stre.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -20.0 °C |
0.562 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)
(discontinued * Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -40.0 °C |
0.562 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)
(discontinued * Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |