Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 19.0 J | 14.0 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 1733HI Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1733HI engineered polyolefin is designed for large, painted automotive exterior applications that require dimensional stability over a broad temperature range. This material e.. |
|||
Impact Test | 19.0 J | 14.0 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 1880 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1880 engineered polyolefin is designed for large automotive applications that require dimensional stability over a broad temperature range. This material exhibits excellent pr.. |
|||
Impact Test | 19.0 J | 14.0 ft-lb | Instrumented Impact Total Energy; ASTM D3763 |
ExxonMobil LD 513.48 Molding, Extrusion and Compounding Resin
(discontinued **) LD 513.48 is a medium MI, low density polyethylene resin designed for use in compounds and masterbatches where its properties ensure improved processability and uniform dispersion of additives. The.. |
|||
Impact Test | 19.0 J @Temperature -29.0 °C |
14.0 ft-lb @Temperature -20.2 °F |
Montell drop weight impact strength |
LyondellBasell Pro-fax SB912 Polypropylene Impact Copolymer Key Features: fully formulated polypropylene copolymer resin, homopolymer-like stiffness wit improved impact strength, resist dust and dirt pick-up, excellent strengthApplications: closures, contain.. |
|||
Impact Test | 19.0 J @Temperature -30.0 °C |
14.0 ft-lb @Temperature -22.0 °F |
Dynatup Impact, E at Max Load, Ductile; ASTM D3763 |
LyondellBasell Hifaxâ„¢ ETA-5061 Thermoplastic Olefin Resin Key Features: fractional melt flow, medium low modulus, blow molding grade thermoplastic olefin resin, flexible, good impact resistance, good processabilityApplications: automotive ductwork, convolu.. |
|||
Impact Test | 19.0 J @Temperature 23.0 °C |
14.0 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl PX7446 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 19.0 J | 14.0 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP PDXF89080 PE LNP* LUBRICOMP* PDXF89080 is a compound based on Polyethylene containing Proprietary Fillers. Added feature of this grade is: Wear Resistant. |
|||
Impact Test | 19.0 J @Temperature 23.0 °C |
14.0 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp TH0450D LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Impact Test | 19.0 J @Temperature 23.0 °C |
14.0 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific) LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Impact Test | 19.0 J | 14.0 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Impact Test | 19.0 J | 14.0 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Impact Test | 19.0 J @Thickness 3.17 mm, Temperature 23.0 °C |
14.0 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ARM impact |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Impact Test | 19.0 J @Thickness 3.17 mm, Temperature 23.0 °C |
14.0 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ARM impact |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Impact Test | 19.0 J @Thickness 3.17 mm, Temperature 23.0 °C |
14.0 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ARM impact |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Impact Test | 19.0 J @Thickness 3.17 mm, Temperature 23.0 °C |
14.0 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ARM impact |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Impact Test | 19.0 J @Thickness 3.17 mm, Temperature 23.0 °C |
14.0 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ARM impact |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Impact Test | 19.0 J @Temperature -20.0 °C |
14.0 ft-lb @Temperature -4.00 °F |
Instrumented Impact Total Energy; ASTM D3763 |
ExxonMobil LD 617.LN Molding, Extrusion and Compounding Resin Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is.. |
|||
Impact Test | 19.0 J | 14.0 ft-lb | @ 73ºF, Instrumented Impact Total Energy; ASTM D3763 |
ExxonMobil LD 637.LI Molding, Extrusion and Compounding Resin Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos.. |
|||
Impact Test | 19.0 J | 14.0 ft-lb | Torque Strength; curing at 1000°F |
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled |
|||
Impact Test | 19.0 J @Thickness 3.17 mm, Temperature 23.0 °C |
14.0 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ARM impact |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Impact Test | 19.0 J | 14.0 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Impact Test | 19.0 J | 14.0 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon MDM40 PP LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region. |