Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy FXTW26SK ASA Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp DFL329EF PC LNP LUBRICOMP* DFL329EF is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.This data was supplied by .. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 1440LS TPO
(discontinued **) Description: SEQUEL® 1440LS engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent processabilit.. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 1718HFLS Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1718HFLS engineered polyolefin is designed for partially painted or molded-in color automotive exterior applications that require very low shrinkage and dimensional stability o.. |
|||
Impact Test | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Asia Pacific) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Asia Pacific region... |
|||
Impact Test | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Europe-Africa-Middle East) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
LyondellBasell SEQUEL® 1480 Engineered Polyolefin Description: SEQUEL® 1480 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent paintability,.. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR (Asia Pacific) LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Impact Test | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications.
Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-LOY KX96821 Acetal LNP STAT-LOY* KX96821 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 (Asia Pacific) LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | Total Penetration Energy; ISO 6603-2 |
Borealis Borpact™ SG321MO Polypropylene Random Heterophasic Copolymer for Injection Molding Borpact SG321MO is a specially designed modified relatively soft and transparent polypropylene random heterophasic copolymer intended for injection molding. Borpact SG321MO has excellent flow, is f.. |
|||
Impact Test | 18.0 J @Thickness 3.17 mm |
13.3 ft-lb @Thickness 0.125 in |
Drop Impact; API |
Total PPH 3727W Polypropylene, High Performance Injection Molding Grade Balanced Properties TOTAL Polypropylene 3727W strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability making it a superior molding grade for.. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | Absorbed energy with 3.5 kN maximum load. 12.7 mm hemisphere insert; 38.1 mm circle support; 5.51 kg weight; 4.47 m/s impact velocity. |
Toyobo Zylon® HM Fiber/Epoxy Matrix Unidirectional Composite Poly(p-phenylene-2,6-benzobisoxazole) (PBO) is a rigid-rod isotropic crystal polymer. Zylon is a new high performance fiber developed by TOYOBO using the latest material science and state of the ar.. |
|||
Impact Test | 18.0 J | 13.2 ft-lb | Rheometric |
DuPont Bexloy® AXW502NC010 Modified Ionomer Resin
(discontinued **) A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers DEXFLEX® 826HS TPO
(discontinued **) Description: DEXFLEX® 826HS is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and.. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers DEXFLEX® 930 TPO
(discontinued **) Description: DEXFLEX® 930 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact propert.. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers DEXFLEX® 930HS TPO
(discontinued **) Description: DEXFLEX® 930HS is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact prope.. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers DEXFLEX® 980HF TPO
(discontinued **) Description: DEXFLEX® 980HF is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact prope.. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON RV00CES PA 66 LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific) LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Impact Test | 18.0 J | 13.3 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural |