Mechanical Properties Metric English Comments
300% Modulus 0.0150 GPa
2.18 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.0150 GPa
2.18 ksi
ISO 37
Huntsman AVALON® 92 AE Thermoplastic Polyurethane
Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi..
300% Modulus 0.0150 GPa
2.18 ksi
DIN 53504
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo..
300% Modulus 0.0150 GPa
2.18 ksi
DIN 53504
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e..
300% Modulus 0.0150 - 0.0210 GPa
2.18 - 3.05 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1502 Styrene Butadiene Rubber
KRALEX® 1502 is a standard grade of styrene butadiene rubber. It is produced by a technology of cold emulsion polymerization based on soaps of rosin and fatty acids and contains 23.5% of chemical..
300% Modulus 0.0150 GPa
2.18 ksi
ASTM D412
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU
Description: Stat-Rite® S1100 is a static dissipative TPU alloy. Stat-Rite S-1100 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD p..
300% Modulus 0.0150 GPa
2.18 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-8290 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0150 GPa
2.18 ksi
ISO 37
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
300% Modulus 0.0150 GPa
2.18 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1685AB Polyester Based TPU
Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0150 GPa
2.18 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.0150 GPa
2.18 ksi
Compounded, 35 mins.; ISO 37
Dynasol Calprene® 1204B Solution Random SBR
Calprene 1204B is a 75/25 Butadiene/Styrene Copolymer, polymerized in solution. It has a random structure with a typical vinyl content of 30%. It is presented in bales wrapped in low melting point p..
300% Modulus 0.0150 GPa
2.18 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1290 Polyester Based TPU
Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd.
Copyright © lookpolymers.com All Rights Reserved