Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0150 GPa | 2.18 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.0150 GPa | 2.18 ksi | ISO 37 |
Huntsman AVALON® 92 AE Thermoplastic Polyurethane Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
300% Modulus | 0.0150 GPa | 2.18 ksi | DIN 53504 |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
300% Modulus | 0.0150 GPa | 2.18 ksi | DIN 53504 |
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
300% Modulus | 0.0150 - 0.0210 GPa | 2.18 - 3.05 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1502 Styrene Butadiene Rubber KRALEX® 1502 is a standard grade of styrene butadiene rubber. It is produced by a technology of cold emulsion polymerization based on soaps of rosin and fatty acids and contains 23.5% of chemical.. |
|||
300% Modulus | 0.0150 GPa | 2.18 ksi | ASTM D412 |
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU Description: Stat-Rite® S1100 is a static dissipative TPU alloy. Stat-Rite S-1100 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD p.. |
|||
300% Modulus | 0.0150 GPa | 2.18 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8290 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0150 GPa | 2.18 ksi | ISO 37 |
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
300% Modulus | 0.0150 GPa | 2.18 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1685AB Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0150 GPa | 2.18 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.0150 GPa | 2.18 ksi | Compounded, 35 mins.; ISO 37 |
Dynasol Calprene® 1204B Solution Random SBR Calprene 1204B is a 75/25 Butadiene/Styrene Copolymer, polymerized in solution. It has a random structure with a typical vinyl content of 30%. It is presented in bales wrapped in low melting point p.. |
|||
300% Modulus | 0.0150 GPa | 2.18 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1290 Polyester Based TPU Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd. |