Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | >= 100 J @Temperature -196 °C |
>= 73.8 ft-lb @Temperature -321 °F |
|
Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel CLC 17-12-2Ti is a Titanium stabilized austenitic stainless steel. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform and localized co.. |
|||
Charpy Impact | >= 100 J @Temperature -196 °C |
>= 73.8 ft-lb @Temperature -321 °F |
|
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c.. |
|||
Charpy Impact | 100 J | 73.8 ft-lb | Typical |
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
Charpy Impact | >= 100 J @Temperature -196 °C |
>= 73.8 ft-lb @Temperature -321 °F |
|
Industeel URANUS® B26 6 Mo High Performance Super-Austenitic Stainless Steel with PREN = 43 Description: URANUS® B26 (UR B26) is a 25% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed for high structural stability and high corr.. |
|||
Charpy Impact | >= 100 J @Temperature -196 °C |
>= 73.8 ft-lb @Temperature -321 °F |
|
Industeel URANUS® B28 High Nickel Super-Austenitic Stainless Steel Description: URANUS® B28 (UR B28) is a super-austenitic stainless steel with very high nickel (31%) and chromium (27%) contents. The molybdenum content is about 3.5%. The alloy is designed for sp.. |
|||
Charpy Impact | >= 100 J @Temperature -196 °C |
>= 73.8 ft-lb @Temperature -321 °F |
|
Industeel URANUS® B6 Multipurpose Austenitic Stainless Steel with PREN = 34 Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t.. |
|||
Charpy Impact | >= 100 J @Temperature -196 °C |
>= 73.8 ft-lb @Temperature -321 °F |
|
Industeel URANUS® B6 N Multipurpose Austenitic Stainless Steel with PREN = 36 Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t.. |
|||
Charpy Impact | >= 100 J @Temperature -196 °C |
>= 73.8 ft-lb @Temperature -321 °F |
|
Industeel URANUS® B66 High Strength Super-Austenitic Stainless Steel with PREN = 54 Description: Research carried out these last five years has shown that combined additions of chromium, tungsten, molybdenum, nitrogen and copper, make it possible to design a super-austenitic stainl.. |
|||
Charpy Impact | 100 J | 73.8 ft-lb | Typical |
Industeel VIRGO 39 16% Cr, 5% Ni, Martensitic Stainless Steel Description: Virgo 39 is a 16% Cr, 5% Ni, 1% Mo low carbon martensitic stainless steel. The grade is specially designed to combine high mechanical properties including toughness and improved corrosi.. |