Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.00 GPa | 290 ksi | ASTM D-638 |
Plaskolite Optix® CA - 900 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ASTM D638 |
Plaskolite Optix® CA-927 Impact Modified Acrylic Resin Injection Molding Grade Pellets. Better impact strength than CA-924. Excellent surface gloss, optical clarity, and practical toughness. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | dry |
Murtfeldt Murdopol® Nylon 12 Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Modulus of Elasticity | 2.00 GPa @Thickness 4.00 mm |
290 ksi @Thickness 0.157 in |
10.0 mm wide molded rod; ISO 178 |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_8210 Rigid Opaque Prototyping Polymer Primary material: VeroBlueSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the .. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_Dots_7513 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_Grid_7523 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet FullCure720 Transparent Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Modulus of Elasticity | 2.00 - 2.60 GPa | 290 - 377 ksi | Average value: 2.35 GPa Grade Count:63 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Modulus of Elasticity | 2.00 - 9.40 GPa | 290 - 1360 ksi | Average value: 5.08 GPa Grade Count:23 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | |
Lehmann & Voss LUVOCOM® 1800-8435 PET, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | |
Lehmann & Voss LUVOCOM® 3-7281/PL/HI/BK Polyamide 6, with PTFE, toughness-modified Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ASTM D790 |
Chengdu Polyster KLX-G42 PC Film & Sheet PC film, high transparency, one side is velvet the other side is matte.Information provided by Chengdu Polyster Co., Ltd. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 20MB666 OPP Film Product Description: Bicor 20MB666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines and is mainly propos.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 21MB777 OPP Film Product Description: Bicor 21MB777 is a high gas barrier, biaxially oriented transparent PP film coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging m.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 35MB666 OPP Film Product Description: A is a biaxially oriented transparent polypropylene film, acrylic coated tow sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle E.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 35LL666 OPP Film Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50LGT702 OPP Film Product Description: A transparent biaxially oriented polypropylene film coated one side resistant coating and one side with a specially formulated acrylic coating. This film is designed for cut and.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50LL210 OPP Film Product Description: An uncoated biaxially oriented, transparent polypropylene film for Pressure Sensitive labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50LL539 OPP Film Product Description: A clear, two-side treated, polypropylene label facestock designed for demanding pressure sensitive applications where outstanding ink adhesion and adhesive anchorage are require.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM388 OPP Film Product Description: A metallized biaxially oriented polypropylene film, metalized on one side with a broad seal range surface on the other side. This film is designed for high barrier performance p.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM483 OPP Film Product Description: A biaxially oriented polypropylene film, metalized on one side with a broad seal range surface on the other side. This film is designed for high barrier performance packaging ap.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM488 OPP Film Product Description: A metalized biaxially oriented polypropylene film, metalized on one side. MM488 is typically used in laminates as the inner web for VFFS and HFFS applications. Due to its slip c.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 17MB400 OPP Film Product Description: Bicor 17MB400 is one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Ou.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 30MBT666 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping, offering unique aspect and cost r.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | In Tension; ASTM D638 |
Devcon Zip Patch™ Epoxy Emergency Repair ProductsComments: High-technology, adhesive-impregnated, putty patching system that cures at room temperature. Hardens to a tough, durable, waterproof finish in minutes. Easy-to-u.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 900 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |