Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 20.7 MPa | 3000 psi | Maximum working pressure |
Potters Industries Q-Cel® 6048 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Compressive Strength | <= 20.7 MPa | <= 3000 psi | Working pressure |
Potters Industries Sphericel® 34P30 Hollow Engineered Glass Microspheres Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Fluorosint® HPV Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Compressive Strength | 20.7 MPa | 3000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet) |
|||
Compressive Strength | 20.7 MPa | 3000 psi | 10% Def.; ASTM D695 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW-PE, Natural & Colored Except Black (ASTM Product Data Sheet) |
|||
Compressive Strength | 20.7 MPa @Temperature 22.8 °C |
3000 psi @Temperature 73.0 °F |
ASTM D695 |
Quadrant EPP TIVAR® 1000 Virgin (Natural & Color except Black) UHMW-PE |
|||
Compressive Strength | 20.7 MPa | 3000 psi | 10% Def.; ASTM D695 |
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Compressive Strength | 20.7 MPa | 3000 psi | 10% Def.; ASTM D695 |
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | 10% Def.; ASTM D695 |
Quadrant EPP TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet) |
|||
Compressive Strength | 20.7 MPa | 3000 psi | 10% Def.; ASTM D695 |
Quadrant EPP TIVAR® Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet) |
|||
Compressive Strength | 20.7 MPa | 3000 psi | 10% Def.; ASTM D695 |
Quadrant EPP TIVAR® H.O.T. UHMW-PE, Premium Heat Stabilized/Anti-Oxidant Filled, (FDA, USDA, & 3-A Dairy) (ASTM Product Data Sheet) |
|||
Compressive Strength | 20.7 MPa | 3000 psi | 10% Def.; ASTM D695 |
Quadrant EPP TIVAR® MD UHMW-PE, FDA Metal Detectable (ASTM Product Data Sheet) Meets FDA and USDA guidelines; 3-A Dairy-approved (natural) Reduces noise Self-lubricating Chemical-, corrosion- and wear-resistant No moisture absorption Non-toxic, low-friction surface Meets ASTM.. |
|||
Compressive Strength | 20.7 MPa @Strain 10.0 %, Temperature 22.8 °C |
3000 psi @Strain 10.0 %, Temperature 73.0 °F |
ASTM D695 |
Quadrant EPP Tivar® Premium UHMW-PE Tivar Premium UHMW-PE |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
SPHERE ONE EXTENDOSPHERESâ„¢ 350 Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
SPHERE ONE EXTENDOSPHERESâ„¢ CG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
SPHERE ONE EXTENDOSPHERESâ„¢ FM-1 Hollow Spheres EXTENDOSPHERESâ„¢FM-1 ceramic hollow spheres are a low-density functional additive for disc brake pads, truck and train blocks, clutch facings and other friction materials. They are compatible wi.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
SPHERE ONE EXTENDOSPHERESâ„¢ HA Hollow Spheres EXTENDOSPHERESâ„¢ HA are off white, low-cost, low-density, high alumina, ceramic hollow spheres.Applications: Hollow spheres are ideal for use in coatings, sealants, caulks and other applications.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
SPHERE ONE EXTENDOSPHERESâ„¢ SG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
SPHERE ONE EXTENDOSPHERESâ„¢ SL-150 Hollow Spheres EXTENDOSPHERESâ„¢ SL are white, low-cost, low-density ceramic hollow spheres.Applications: With a density of 0.73 g/cc and a crush strength of 3,000 psi, these hollow spheres are ideal for use in.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
SPHERE ONE EXTENDOSPHERESâ„¢ SLG Hollow Spheres EXTENDOSPHERESâ„¢ SL are white, low-cost, low-density ceramic hollow spheres.Applications: With a density of 0.73 g/cc and a crush strength of 3,000 psi, these hollow spheres are ideal for use in.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | Service Pressure |
Trelleborg AEM Eccofloat® TG-24/2000 Syntactic Foam TG Grade syntactic foams are lightweight and economical for building manned and remote operating vehicles. The foams are also used to manufacture mine neutralization systems because of their zero ma.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
Cotronics Resbond™ 906 High Temperature Ceramic Adhesive, High Expansion |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
Cotronics Resbond™ 908 High Temperature Ceramic Adhesive, Moisture Proof |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
Cotronics Resbond™ 931 High Temperature Graphite Adhesive |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
Cotronics Resbond™ 989 High Temperature, High Purity Alumina Adhesive, General Purpose |
|||
Compressive Strength | 20.7 MPa | 3000 psi | ultimate load |
BNZ Materials Marinite® A Ceramic Board for Aluminum Contact These boards are heat treated formulations for use in conveying, containing and forming molten aluminum and other non-ferrous metals. Applications include holding furnace linings, tips for continuou.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
3M HGS3000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
3M K37 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Compressive Strength | 20.7 MPa | 3000 psi | |
3M S35 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Compressive Strength | 20.7 - 27.6 MPa | 3000 - 4000 psi | |
Abatron AboCast 7802-1/AboCure 7804-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |