| Category | Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | TIVAR® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Quadrant EPP TIVAR® 1000 Virgin (Natural & Color except Black) UHMW-PE.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.930 g/cc @Temperature 22.8 °C |
0.930 g/cc @Temperature 73.0 °F |
ASTM D792 |
| Water Absorption at Saturation | 0.010 % | 0.010 % | ASTM D570 2 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 66 @Temperature 22.8 °C |
66 @Temperature 73.0 °F |
ASTM D2240 |
| Tensile Strength | 40.0 MPa @Temperature 22.8 °C |
5800 psi @Temperature 73.0 °F |
ASTM D638 |
| Tensile Modulus | 0.552 GPa @Temperature 22.8 °C |
80.0 ksi @Temperature 73.0 °F |
ASTM D638 |
| Flexural Strength | 24.1 MPa @Temperature 22.8 °C |
3500 psi @Temperature 73.0 °F |
ASTM D790 |
| Compressive Strength | 20.7 MPa @Temperature 22.8 °C |
3000 psi @Temperature 73.0 °F |
ASTM D695 |
| Compressive Modulus | 0.552 GPa @Temperature 22.8 °C |
80.0 ksi @Temperature 73.0 °F |
ASTM D695 |
| Shear Strength | 33.1 MPa @Temperature 22.8 °C |
4800 psi @Temperature 73.0 °F |
ASTM D732 |
| Coefficient of Friction, Dynamic | 0.12 | 0.12 | QTM 55007 |
| Sand Slurry | 10 | 10 | 1018 Steel = 100; ASTM D4020 |
| Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | (with 4:1 safety factor applied); QTM 55007 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.409 W/m-K | 2.84 BTU-in/hr-ft²-°F | ASTM E 1530-11 |
| Melting Point | 135 °C | 275 °F | ASTM D3418 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 45.3 kV/mm | 1150 kV/in | ASTM D149 |