Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added features include: Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC (Asia Pacific) LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific) LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp DF0069E PC LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC.. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp DF0069E PC (Asia Pacific) LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC.. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP SF008 PA 12 LNP* THERMOCOMP* SF008 is a compound based on Nylon 12 resin containing 40% Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP UF009S PPA LNP THERMOCOMP* UF009S is a compound based on Polyphthalamide resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Asia Pacific) LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Asia Pacific) LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East) LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP SF008 PA 12 (Asia Pacific) LNP* Thermocomp* SF008 is a compound based on Nylon 12 resin containing Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 (Asia Pacific) LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0018 cm/cm @Time 86400 sec |
0.0018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 (Asia Pacific) LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |