Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE)
The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, A..
Melt Flow 9.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
9.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
SABIC FJ00952 High Density Polyethylene for Blown Film
Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, ..
Melt Flow 9.0 - 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 - 13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 2062U (62111) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 9.0 - 12.6 g/10 min

@Load 21.6 kg,
Temperature 190 °C
9.0 - 12.6 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 6748F (486H6) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 9.0 - 12.6 g/10 min

@Load 21.6 kg,
Temperature 190 °C
9.0 - 12.6 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 6749F (486H6) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Asia Pacific)
Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® IR2240 PC
UL rated HB. 200 series recommended when V-2 rating required. Nonhalogenated. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle ..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® SLX1482T PC Copolymer
Medium viscosity PC Copolymer, enhanced UV stabilization. Transprarent and tinted colors. Higher mold release content than SLX1432T.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was suppli..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer
Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® SLX1482T PC Copolymer (Asia Pacific)
Medium viscosity PC Copolymer, enhanced UV stabilization. Transprarent and tinted colors. Higher mold release content than SLX1432T.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-M..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics PC1000 PC (Asia Pacific)
PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics PC1000 PC (Europe-Africa-Middle East)
PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics PC1000R PC (Asia Pacific)
PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics PC1003R PC
PC1003R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was ..
Melt Flow 9.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Styrolution Novodur® 4105 ABS
Novodur Ultra 4105 is a PC modified high heat injection molding grade with high impact strength.Information provided by Styrolution
Melt Flow 9.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Styrolution Novodur® 4140PG ABS
Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by ..
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 260 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 220 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 428 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Melt Flow 9.0 - 13 g/10 min

@Load 3.80 kg,
Temperature 230 °C
9.0 - 13 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 3501 SHF
Description: Super High FlowInformation provided by Diamond Polymers, Inc.
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 220 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 428 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 220 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 428 °F
ISO 1133
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved