Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 200 °C |
16 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, A.. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 220 °C |
16 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® INP562 ABS SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 220 °C |
16 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® INP572 ABS High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 220 °C |
16 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® S702S ABS (Europe-Africa-Middle East) CYCOLAC S702S is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries. Cycolac S702S is anti-dust equiped.. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 220 °C |
16 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® S702S ABS (Europe-Africa-Middle East) CYCOLAC S702S is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries. Cycolac S702S is anti-dust equiped.. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 250 °C |
16 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 250 °C |
16 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Melt Flow | 16 - 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
16 - 20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 2060V (60118) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS2S PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® ML7678 PC 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regio.. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 260 °C |
16 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East) XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 200 °C |
16 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G2780C Thermoplastic Elastomer (TPE) Dynaflex™ G2780C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmold A.. |
|||
Melt Flow | 16 - 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
16 - 20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4052V (52418) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 360 °C |
16 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1100EF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 360 °C |
16 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 360 °C |
16 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 220 °C |
16 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Melt Flow | 16 g/10 min @Load 6.60 kg, Temperature 337 °C |
16 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1110FV PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data was supplied by SABIC-I.. |
|||
Melt Flow | 16 g/10 min @Load 6.60 kg, Temperature 337 °C |
16 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1110V PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 360 °C |
16 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 250 °C |
16 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 250 °C |
16 g/10 min @Load 11.0 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 260 °C |
16 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® APC100 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 300 °C |
16 g/10 min @Load 11.0 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East) High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |