Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 260 °C |
12 g/10 min @Load 4.76 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 12 g/10 min @Load 10.0 kg, Temperature 220 °C |
12 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
SABIC Innovative Plastics Geloy FXTW26SK ASA Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 12 g/10 min @Load 10.0 kg, Temperature 220 °C |
12 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 12 - 30 g/10 min @Load 21.6 kg, Temperature 190 °C |
12 - 30 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio 30-50; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4143L (424F5) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 12 g/10 min @Load 3.80 kg, Temperature 230 °C |
12 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® IFX2420Z PC (Asia Pacific) Lexan* IFX2420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware applications specifically for welding. This grades .. |
|||
Melt Flow | 12 g/10 min @Load 1.20 kg, Temperature 250 °C |
12 g/10 min @Load 2.65 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® ML1010 PC (Europe-Africa-Middle East) Superior performance, improved flow over standard grades at lower temperatures. Internal mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 12 g/10 min @Load 5.00 kg, Temperature 190 °C |
12 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MM 74 High Density Polyethylene - Injection Molding Eraclene MM 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 74 is characterized by a good balance between rigidity and impact.. |
|||
Melt Flow | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific) DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r.. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Moplen HP400N Polypropylene Homopolymer Description: HP400N is a high flow homopolymer with a conventional molecular weight distribution and is formulated with a general-purpose additive package. HP400N is designed for injection molding a.. |
|||
Melt Flow | 12 g/10 min @Load 10.0 kg, Temperature 220 °C |
12 g/10 min @Load 22.0 lb, Temperature 428 °F |
Index; ASTM-D1238 |
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)... |
|||
Melt Flow | 12 g/10 min @Load 21.6 kg, Temperature 190 °C |
12 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene EX3-80 is a high density polyethylene with 1-Butene as co monomer. It is natural, good ESCR, good impact strength, tough and rigid pipe resin. Applications: pipe extrusion PE 80 class, industrial a.. |
|||
Melt Flow | 12 g/10 min @Load 5.00 kg, Temperature 210 °C |
12 g/10 min @Load 11.0 lb, Temperature 410 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Melt Flow | 12 g/10 min @Load 5.00 kg, Temperature 250 °C |
12 g/10 min @Load 11.0 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 265 °C |
12 g/10 min @Load 4.76 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Europe-Africa-Middle East) Mold Release version of X7200This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 265 °C |
12 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Asia Pacific) PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 12 g/10 min @Load 5.00 kg, Temperature 200 °C |
12 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution Styrolux 3G33 SBC Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and .. |
|||
Melt Flow | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® CF-1051 PC, Unreinforced High Impact High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 265 °C |
12 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled Daplen EE137AI is a 10% mineral filled grade intended for injection molding. EE137AI has been developed especially for the car industry, to be used in interior parts where high scratch resistance i.. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis ME266U Polypropylene Compound, Mineral Filled ME266U is a 20% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. .. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis ME212U Polypropylene Compound, Mineral Filled ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air.. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
12 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Melt Flow | 12 g/10 min @Load 3.80 kg, Temperature 230 °C |
12 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers NPP 808 C2 TDS Polycarbonate Alloy, Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
12 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
12 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Melt Flow | 12 g/10 min @Load 5.00 kg, Temperature 200 °C |
12 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total Lacqrene® 852 High Impact Polystyrene
(discontinued **) LACQRENE® 852 is a flame retardant, high impact polystyrene, halogen free, with excellent thermal stability.ApplicationCopier, Fax, Printers, Television, decoders, Hi-FiInformation provided provide.. |
|||
Melt Flow | 12 g/10 min @Load 8.70 kg, Temperature 190 °C |
12 g/10 min @Load 19.2 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Elastamax HTE 2101-1002 Polyurethane Alloy
(discontinued **) This is an extrusion grade polyurethane alloy. Physical Form: Pellet. Standard Color: Off white, opaque.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. .. |
|||
Melt Flow | 12 g/10 min @Load 5.00 kg, Temperature 280 °C |
12 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 265 °C |
12 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Asia Pacific region. |