Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers Softflex® 5300 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers Softflex® 5500 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 210 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis BorPURE™ RB501BF Polypropylene Copolymer BorPure™ RB501BF is a random copolymer. Applications: BorPure™ RB501BF has been developed especially for applications like: food packaging, over wrap film, label film, and shrink film. Additives.. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg |
1.9 g/10 min @Load 11.0 lb |
ASTM D 1238 |
Total 8183 HDPE, blow molding Applications: cosmetic bottles, pharmaceutical bottles, industrial product containers, chemical packaging, food packagingInformation provided provided by Total Petrochemicals.Total Petrochemicals ac.. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
Total HDPE 7194 High Density Polyethylene, Specialty Extrusion Resin Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationUSP Class VI compliantApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformat.. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
Total HDPE 7195 High Density Polyethylene, Specialty Extrusion Resin Characteristics:Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformation pr.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal (POM)
(Unverified Data**) Nucleated High Viscosity Acetal Homopolymer Developed for Extrusion Delrin 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability low die deposi.. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Denka STYROL MW1 Polystyrene "DENKA SYTROL MW" is a well-balanced polystyrene (PS) resin, with a high tensile strength as well as good moldability. Overturning the traditional understanding that PS resin is "hard and brittle," .. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Denka STYROL MW1 Polystyrene "DENKA SYTROL MW" is a well-balanced polystyrene (PS) resin, with a high tensile strength as well as good moldability. Overturning the traditional understanding that PS resin is "hard and brittle," .. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Melt Flow | 1.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 7501 E Description: Extrusion Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS TM 25 Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA S319 Description: ASA Weatherable Polymer, Injection Molding Grade, High ModulusInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Polylac® PA-707 ABS High gloss, high rigid |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact ApplicationsDelrin FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. I.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Denka TX-100S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Styrolution NAS® 21 Acrylic Copolymer Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma.. |