Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.5 - 2.2 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.5 - 2.2 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polyplastic Torlen® PE 2K 901 High Density Polyethylene, Carbon Filled Information provided by PolyPlastic Group. |
|||
Melt Flow | 1.5 g/10 min @Load 1.00 kg, Temperature 235 °C |
1.5 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 4500 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylac® GP55 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PE 1304
(discontinued **) PRE-ELEC PE 1304 is a conductive thermoplastic compound based on a blend of PE-LD/PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivi.. |
|||
Melt Flow | 1.5 - 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.5 - 2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
±10% |
Kazanorgsintez PE2NT 17-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene G2855 High Density Polyethylene CHARACTERISTICS:GOOD IMPACT STRENGTH, MEDUIM STIFFNESSGOOD PROCESSABILITYAPPLICATIONS:BLOW MOLDINGFOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES,COSMETIC BOTTLES, CHEMICAL CONTAI.. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene G2865 High Density Polyethylene CHARACTERISTICS: HIGH STIFFNESS, GOOD IMPACT STRENGTH, GOOD PROCESSABILITYAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DIARY PRODUCT BOTTLES, FRUIT JUICE BOTTLES, ONE-.. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene GM2865 High Density Polyethylene CHARACTERISTICS: EXCELLENT STIFFNESS, GOOD PROCESSABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DAIRY PRODUCT BOTTLES MILK BOTTLES AND GALL.. |
|||
Melt Flow | 1.5 - 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.5 - 2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
±10% |
Kazanorgsintez PE2NT 17-5 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Melt Flow | <= 1.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
<= 1.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
MTM Plastics Purpolen® PE Polyethylene Regrind Purpolen® is a sorted regrind material suited to the production of demanding end user products. Extrusion and injection molding grades are available in many colors. The basis of our Purpolen® .. |
|||
Melt Flow | 1.5 - 2.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.5 - 2.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Lushan L-5R (F) Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |
|||
Melt Flow | 1.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS 8014 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM Test |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Melt Flow | 1.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
1.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ISO 1133 |
Polyplastics TOPAS® 6017 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Possesses the highest heat resistance among cyclic olefin-type resins.Information provided by PolyPlastics. |
|||
Melt Flow | 1.5 - 3.5 g/10 min @Load 2.16 kg, Temperature 180 °C |
1.5 - 3.5 g/10 min @Load 4.76 lb, Temperature 356 °F |
|
Wacker Silicones Geniomer® 140 Silicone TPE SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Kibisan® PN-127 SAN Heat Resistant |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 4501 Injection Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 1.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS TM 40 Description: Heat Resistant Grade, Ultra High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS/PC FC-30 Description: Injection Molding Grade, High Impact, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABSPC 7030 ABS/PC Injection Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA S140 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA S510 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA/PC TA-35 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Kibisan® PN-127H SAN Chemical Resistant |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Denka TX-600S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Melt Flow | 1.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY VP22 NATURAL 1001B Blow Molding Grade, Flame Retardant ABS Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 1.5 - 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.5 - 3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene SPM Thermoplastic Composite, 70% HD + 30% PP Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 230 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Melt Flow | 1.5 - 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.5 - 3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Breplast Bretene SPF Thermoplastic Composite, 40% PP + 60% PE Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |