Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.1 g/10 min @Load 1.00 kg, Temperature 235 °C |
1.1 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 5000 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 1.1 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.1 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers Softflex® 7200 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 1.1 g/10 min @Load 10.0 kg, Temperature 190 °C |
1.1 g/10 min @Load 22.0 lb, Temperature 374 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE.. |
|||
Melt Flow | 1.1 g/10 min @Load 5.00 kg |
1.1 g/10 min @Load 11.0 lb |
ISO 1133 |
Total Lacqtene® 2004 TN 52 HDPE pipe
(discontinued **) LACQTENE® 2004 TN 52 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2004 TN 52 is best processed between 190 and 230°C.Informa.. |
|||
Melt Flow | 1.1 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.1 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) BL2 HF 4750 High Density Polyethylene BL2 is a high density polyethylene with 1-Butene as co monomer. It is high impact strength and slightly, lower stiffness than BL3, outstanding resistance to stress cracking, even in contact with su.. |
|||
Melt Flow | 1.1 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.1 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Test |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Melt Flow | 1.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 3501 Black 1302 Injection Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 1.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3501 GF-10 Description: Reinforced Grade, 10%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.1 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.1 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA T-105 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.1 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.1 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA T-110 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.1 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.1 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA T-115 Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.1 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.1 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA TW-20 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |