Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon A3020-R008-16.5 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
&nb 2 inches width and 50 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Th.. |
|||
Thickness | 203 - 254 microns | 8.00 - 10.0 mil | Overall |
Arlon 48571R009 0.009" (0.229 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate |
Arlon 51426R015 0.015" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the productio.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon 51571XC015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 203 microns | 8.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51576R024A 0.024" (0.610 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon 51576S020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 203 - 229 microns | 8.00 - 9.00 mil | Side 1 |
Arlon 51576S020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 51579XA028 0.028" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material a.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 51586R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clot.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon 51591R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data .. |
|||
Thickness | 203 microns | 8.00 mil | Side 2, Layer 2; Arlon SQA-TMS-003 |
Arlon 55578R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Appearance:.. |
|||
Thickness | >= 203 microns | >= 8.00 mil | Side 2, Uncured |
Arlon 55578XD028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers Appearance: Gray silicone gum and/or rubber on fiberglass clothThis data Represents typical values for the production ma.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated Polyester Fabric, Substrate |
Arlon 70011B016 0.016" (0.406 mm) Uncured Silicone Rubber with Prime Coated Polyester Fabric Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon P29609R015 0.015" (0.381 mm) Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer Product Use: Traction motor insulation, electrical insulationAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the pr.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon R32089R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-012 |
Arlon T4020-R002 0.020" Cured, Fusible Silicone Rubber with Fiberglass Substrate 0.5 inch wide, 20 mil thick, red, rectangular cross-section, fusible silicone tape.Design/Construction:Side 1: Cured Fusible Silicone RubberSubstrate: 15% Sinusoidal FiberglassSide 2: Cured Fusibl.. |
|||
Thickness | 203 microns | 8.00 mil | Overall; Arlon SQA-TMS-003 |
Arlon Thermabond® 99A90X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Thickness | 203 microns | 8.00 mil | Overall |
Arlon Thermabond®-II 99760N008 0.008" (0.203 mm) Unsupported/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Unsupported/Uncured RubberAppearance: White/gray gumAppearance: White/grey gumThis data Represents typical values for the production material. The data should not be used.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 51103R015 0.0150" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: LDPEThis data represents typical values for the producti.. |
|||
Thickness | 203 microns | 8.00 mil | substrate; Arlon SQA-TMS-003 |
Arlon 51276R015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 51279R020 0.020" (0.508 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass This data represents typical values for the production ma.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon 51420R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate |
Arlon 51561R015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the .. |
|||
Thickness | 203 microns | 8.00 mil | Substrate |
Arlon 51581R018 0.018" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon 51946C015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon 51970R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, or .. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon R33991R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon R35798R013 0.013" (0.330 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 Fiberglass Side 2: Uncured Silicone RubberThis data represents typic.. |
|||
Thickness | 203 microns | 8.00 mil | |
3M Scotch® 2520 Varnished Cambric Tape Scotch® Varnished Cambric Tapes are made from straight-cut woven cotton cambric fabric. The fabric is oil primed and coated with a high-grade yellow electrical insulating varnish. Varnished cambric.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon R35928R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |