3M Scotch® 2520 Varnished Cambric Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 2520 Varnished Cambric Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Scotch® Varnished Cambric Tapes are made from straight-cut woven cotton cambric fabric. The fabric is oil primed and coated with a high-grade yellow electrical insulating varnish. Varnished cambric tapes are flexible, electrically insulating and moisture resistant with a smooth finish. 2510 tape is yellow, non-adhesive coated and 7 mils thick. 2520 tape is yellow with a pressure-sensitive adhesive and 8 mils thick. They are designed to perform continuously in temperatures up to 105°C with excellent resistance to abrasion, puncture and cut-through. The adhesive on 2520 tape holds the tape in position after application.Information provided by 3M
Physical Properties Metric English Comments
Thickness 203 microns
8.00 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 43.1 MPa
6250 psi
ASTM D295
Peel Strength 0.0877 kN/m
0.500 pli
Adhesion to Backing; ASTM D1000
0.1424 kN/m
0.8125 pli
Adhesion to Steel; ASTM D1000
Electrical Properties Metric English Comments
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D295
Descriptive Properties Value Comments
Appearance Yellow