Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 356 microns | 14.0 mil | Per Ply |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K 8HS Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Thickness | 356 - 1270 microns | 14.0 - 50.0 mil | |
Alcoa KAMA Petwich-PET 4300 Petwich-PET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Recycled contentSi.. |
|||
Thickness | 356 microns | 14.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R35551X014 0.014" (0.356 mm) Uncured Rubber with Coated Nextel Substrate
(discontinued **) Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberSubstrate: Coated Nextel This data Represents typical values for the production material. The data should not be used to write, or in .. |
|||
Thickness | 356 microns | 14.0 mil | |
Hexcel® HexForce™ 332 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 356 microns | 14.0 mil | |
Hexcel® HexForce™ 232 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 356 microns | 14.0 mil | Nominal |
DuPont™ Nomex® 418 Paper, 14 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Thickness | 356 microns | 14.0 mil | Typical; ASTM D374 |
DuPont™ Nomex® 418 Paper, 14 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Thickness | 356 microns | 14.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 19146R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Black silicone gum and rubber on fiberglass clothT.. |
|||
Thickness | 356 microns | 14.0 mil | Prime Coated 1523 Fiberglass, Substrate |
Arlon 19562R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wr.. |
|||
Thickness | 356 microns | 14.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 19563R032 0.032" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Cured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the producti.. |
|||
Thickness | >= 356 microns | >= 14.0 mil | Prime Coated 1523 Fiberglass, Substrate |
Arlon 19566R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The.. |
|||
Thickness | 356 microns | 14.0 mil | Prime Coated 1523 Fiberglass, Substrate |
Arlon 19571R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 356 microns | 14.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the production mat.. |
|||
Thickness | 356 microns | 14.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 19606R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 1523 FiberglassSide 2: Uncured Silicone RubberInterleave: 0.003" PolyethyleneThis data represents typical values for the .. |
|||
Thickness | 356 - 406 microns | 14.0 - 16.0 mil | Overall |
Arlon 30560R015 0.015" (0.381 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Thickness | 356 microns | 14.0 mil | Layer 1; Arlon SQA-TMS-003 |
Arlon 61089R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Denier Vectran HS Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 1000 Denier HS Appearance: Red silicone gum on fabricThis data represents t.. |
|||
Thickness | 356 microns | 14.0 mil | Nominal |
AK Steel CARLITE® M-6 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Thickness | 356 - 406 microns | 14.0 - 16.0 mil | Overall |
Arlon P29609R015 0.015" (0.381 mm) Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer Product Use: Traction motor insulation, electrical insulationAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the pr.. |
|||
Thickness | 356 microns | 14.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R34381R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 7628 Style FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typical.. |
|||
Thickness | 356 microns | 14.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R34591R014 0.014" (0.356 mm) Uncured Silicone Rubber Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 2116 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicon.. |
|||
Thickness | 356 - 406 microns | 14.0 - 16.0 mil | Overall |
Arlon R34661R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 356 microns | 14.0 mil | Prime Coated 11523 Fiberglass, Substrate |
Arlon R34896R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 356 microns | 14.0 mil | Prime Coated 1523 Fiberglass, Substrate |
Arlon 19096R022 0.022" (0.559 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place of,.. |
|||
Thickness | 356 - 406 microns | 14.0 - 16.0 mil | Overall |
Arlon 51576X015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 356 microns | 14.0 mil | Prime Coated 2523 Fiberglass, Substrate |
Arlon R31246R060 0.060" (1.52 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate.. |
|||
Thickness | 356 microns | 14.0 mil | Prime Coated 2523 Fiberglass, Substrate |
Arlon R31246R063 0.063" (1.60 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate.. |
|||
Thickness | 356 microns | 14.0 mil | Prime Coated 2523 Fiberglass, Substrate |
Arlon R34256R063 0.063" ((1.60 mm) Uncured/Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate.. |
|||
Thickness | 356 - 457 microns | 14.0 - 18.0 mil | Caliper |
3M Diamond Grade™ 983 Conspicuity Markings 3M™ Diamond Grade™ Conspicuity Markings Series 983 are highly retrorflective micro-prismatic markings designed to mark the sides and rear of vehicles for enhanced visibility and detection. The ref.. |
|||
Thickness | 356 microns | 14.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R36461R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Liner: Polyethylene This data represents typical values for.. |
|||
Thickness | 356 microns | 14.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib.. |