Polymer Property : Thickness = 50.0 mil Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Thickness 635 - 1270 microns
25.0 - 50.0 mil
Range of Thicknesses Available
Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate
Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel..
Thickness 635 - 1270 microns
25.0 - 50.0 mil
Range of Thicknesses Available
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate
Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel..
Thickness 178 - 1270 microns
7.00 - 50.0 mil
Alcoa KAMA 4100 Prime APET  (discontinued **)
CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Available in clear,..
Thickness 178 - 1270 microns
7.00 - 50.0 mil
Alcoa KAMA 4200 RPET  (discontinued **)
CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Up to 100% recycled..
Thickness 356 - 1270 microns
14.0 - 50.0 mil
Alcoa KAMA Petwich-PET 4300 Petwich-PET  (discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Recycled contentSi..