Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.3 g/10 min | 5.3 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE D 4308 BLK The moisture content is 0.04%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 5.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin
(discontinued **) Features: Octene co-polymer, excellent sealability and toughness, high drawdown, high adhesion, good barrier, good abrasion resistance.Applications: Food packaging, milk cartons, paperboard containe.. |
|||
Melt Flow | 5.3 g/10 min @Load 2.16 kg, Temperature 250 °C |
5.3 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High Impact.Application: Automotive (Interior), E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 5.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
old Condition G; ASTM D1238 |
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Melt Flow | 5.3 - 10.3 g/10 min @Load 1.20 kg, Temperature 250 °C |
5.3 - 10.3 g/10 min @Load 2.65 lb, Temperature 482 °F |
|
Kazanorgsintez PC-075DA Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for manufacture of optical products by method of die-casting (including CD, DVD, and other discs), as well .. |
|||
Melt Flow | 5.3 g/10 min @Load 6.60 kg, Temperature 337 °C |
5.3 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2300R PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 5.3 g/10 min @Load 6.60 kg, Temperature 337 °C |
5.3 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2300R PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 5.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® HG-0760LT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 5.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® HG-0760LT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 5.3 g/10 min @Load 5.00 kg, Temperature 280 °C |
5.3 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PN275 PPE+PS PPE+PS with low mineral loading. High heat, platable applications. |
|||
Melt Flow | 5.3 g/10 min @Load 5.00 kg, Temperature 280 °C |
5.3 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PN275F PPE+PS PPE+PS with low mineral loading. High heat, platable applications. NSF approved for water contact applications. |
|||
Melt Flow | 5.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPH 5069 Polypropylene Homopolymer, Fiber Polypropylene PPH 5069 is a homopolymer polypropylene with a Melt Flow index of 6 g/10 min.Polypropylene PPH 5069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Melt Flow | 5.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® 4053FG TPC-ET
(Unverified Data**) Hytrel® 4053FG is a low modulus high performance thermoplastic elastomer with food compliance specificity. It is suitable for extrusion and injection molding processes.Information provided by DuPon.. |
|||
Melt Flow | 5.3 g/10 min @Load 2.16 kg, Temperature 235 °C |
5.3 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Conditioned) Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to .. |
|||
Melt Flow | 5.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics STYRON™ 668 General Purpose Polystyrene Resin STYRON™ 668 is a general purpose polystyrene with medium flow and a balance of heat resistance and stiffness characteristics that make it suitable for applications such as CD jewel boxes. STYRON™.. |
|||
Melt Flow | 5.3 g/10 min @Load 2.16 kg, Temperature 235 °C |
5.3 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Dry) Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to .. |
|||
Melt Flow | 5.3 g/10 min @Load 2.16 kg, Temperature 235 °C |
5.3 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Dry) Designation ISO 1874-PA12/xx,MHLR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good.. |