Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 28 g/10 min | 28 g/10 min | ASTM D1238 |
Mytex Polymers AS33L(W)-06 Polypropylene, Rubber modified, Talc filled, Compounded Description: AS33L(W)-06 is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and .. |
|||
Melt Flow | 28 g/10 min @Load 6.60 kg, Temperature 400 °C |
28 g/10 min @Load 14.6 lb, Temperature 752 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM UH1026 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent |
|||
Melt Flow | 28 g/10 min @Load 1.20 kg, Temperature 300 °C |
28 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Melt Flow | 28 g/10 min @Temperature 230 °C |
28 g/10 min @Temperature 446 °F |
ISO 1133 |
Phillips Sumika Marlex® CHP-275 Thermoplastic Polyolefin
(discontinued **) Engineered Thermoplastic Polyolefin.Applications: Automotive Head and Side Impact TrimConditioning after Molding: 48 hr at 23°C, 48 hr at 90°CNominal Shrinkage: 0.7-0.9%, 0.8-1.1%Drying conditions.. |
|||
Melt Flow | 28 g/10 min | 28 g/10 min | ISO 1133 |
Solvay Engineered Polymers SEQUEL® 1492 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1492 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent p.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 260 °C |
28 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 220 °C |
28 g/10 min @Load 22.0 lb, Temperature 428 °F |
JIS K7210 |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman M3018-P Polyethylene
(discontinued **) Low density polyethylene M3018-P is a specialty formulation suggested for low temperature extrusion coating applications. M3018-P has been found to exhibit good coatability and adhesion to various .. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 250 °C |
28 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
LG Chemical LUPOY GN5001RFT PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Iran Petrochemical (PCC) 52528 High Density Polyethylene 52528 is a HDPE copolymer injection molding grade for thin walled applications requiring a good balance between high flowability and physical properties.Application: caps, thin walled, injection mol.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 270 °C |
28 g/10 min @Load 11.0 lb, Temperature 518 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Melt Flow | 28 g/10 min | 28 g/10 min | ASTM D1238 |
Hyosung Topilene J742S PP J742S Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corpora.. |
|||
Melt Flow | 28 g/10 min @Load 1.20 kg, Temperature 300 °C |
28 g/10 min @Load 2.65 lb, Temperature 572 °F |
Can be modified between 10 and 20 g/10mins; ASTM D1238 |
MRC Polymers NAXELLâ„¢ PC23MS Polycarbonate, Impact Modified, High MFR, EZ Flow Economy GradeImpact modifiedCan be UV stabilizedGenerally for black onlyInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 250 °C |
28 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HP-1000XA PC/ABS, Unreinforced PC/ABS material for automobile IP-coreInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 250 °C |
28 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® VB-5305G PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 250 °C |
28 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HP-1000XA PC/ABS, Unreinforced PC/ABS material for automobile IP-coreInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 28 g/10 min @Load 3.80 kg, Temperature 260 °C |
28 g/10 min @Load 8.38 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL N750 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business Equipment applications. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3015 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3015 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3015 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3015 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3015 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3015 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 260 °C |
28 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
Cossa Polimeri ESTABLEND 4501 V0/D Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, PBDE and antimony free, with halogens, high impact resistance, very high thermal resistance, high gloss, good processabilityInformation provided by Cossa Poli.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 265 °C |
28 g/10 min @Load 11.0 lb, Temperature 509 °F |
cm³/10 min. |
Covestro Makroblend® UT-400 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 265 °C |
28 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
Diamond Polymers ABSPC 9802 ABS/PC Molding Grade, High Impact, High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 28 g/10 min | 28 g/10 min | ISO 1133 |
Addiplast Addilene H 652 Polypropylene Homopolymer High temperature resistance, high gloss, very good surface appearanceInformation provided by Addiplast. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 200 °C |
28 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
BASF Polystyrol® 144 C Polystyrene (Europe) Very easy flowing grade, often blended with impact-modified Polystyrol or used as a coextruded glossy layer.Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 220 °C |
28 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Polylac® PA-763A ABS - Flame Retardant F.R. High Heat |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 230 °C |
28 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H28U-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Radiation stableTypical applications: MedicalComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |