Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 19 g/10 min | 19 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Pro® 3018 CU Dark Green 30% Filler Content Polypropylene Data provided by Multibase. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 260 °C |
19 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 300 °C |
19 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 3413R PC (Asia Pacific) Lexan* resin 3413R is a flame retardant polycarbonate grade with 30% glass fiber reinforcement to meet UL 94 V1 listing at 1.5mm. This grade can be considered for applications requiring higher stiff.. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 8111 LLDPE Injection Molding Resin
(discontinued **) Features: Good processability, excellent impact resistance, excellent flexibility and freedom from warpage.Applications: Automotive splash-guards, large containers, closures and lids for food applic.. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® HD-6705 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Medium Flow, Good Stiffness, Good ImpactUses: Food containers, Housewares, Toys |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer 19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 330 °C |
19 g/10 min @Load 4.76 lb, Temperature 626 °F |
|
Covestro Apec® DP 1-9359/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Melt Flow | 19 g/10 min | 19 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® J-60/20/TT/FD WT8381 Polypropylene Homopolymer, 20% Glass Reinforced, FDA compliant Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
Ineos ABS Lustran® PG 298 Key Features:UnfilledPlatableSuitable processing methods:Injection molding |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 230 °C |
19 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H19G-01 Polypropylene Homopolymer Grade H19G-01 is a polypropylene homopolymers designed for extrusion processing and meet the requirements of the U.S. Food and Drug administration as specified in 12 CFR 177.1520.Applications:Contin.. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 260 °C |
19 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/ABS FR 6206 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 260 °C |
19 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/ABS FR 6206 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 250 °C |
19 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® UF-1017 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Styron EMERGEâ„¢ 4850-19 Polycarbonate EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Melt Flow | 19 g/10 min | 19 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman. |
|||
Melt Flow | 19 g/10 min | 19 g/10 min | ASTM D1238 |
Chase Plastics CP Pryme® PC100RHF Polycarbonate Form: PelletsInformation provided by Chase Plastics. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Bright White P80514PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80514PF is a bright white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and molding .. |
|||
Melt Flow | 19 g/10 min @Temperature 230 °C |
19 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 4101O BCF Fiber Spinning Polypropylene HomopolymerApplications: Multifilament and bulk continuous filament fiber.Formolene 4101O is a low viscosity, highly isotactic polypropylene homopolymer designed primarily for multifilament and bulk.. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 350 Ethylene Vinyl Acetate DuPont™ Elvax® 350 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 350 resins can be used for the following applications: .. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 1954 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Low viscosity• UV st.. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 230 °C |
19 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil PP7694E2 Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for applications requiring long-term heat-agi.. |
|||
Melt Flow | 19 g/10 min @Load 3.80 kg, Temperature 230 °C |
19 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diapolyacrylate Acrypet® VH-001 Heat Stabilized PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |
|||
Melt Flow | 19 g/10 min | 19 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Copolymer CP0437M10L Mica Reinforced |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 250 °C |
19 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Asia International Enterprise (Hong Kong) 30G3F Polybutylene terephthalate, 15% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Melt Flow | 19 - 35 g/10 min @Load 3.80 kg, Temperature 232 °C |
19 - 35 g/10 min @Load 8.38 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Melt Flow | 19 g/10 min | 19 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 250 °C |
19 g/10 min @Load 11.0 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East) VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 230 °C |
19 g/10 min @Load 4.76 lb, Temperature 446 °F |
from MVR; ISO 1033 |
Sax Polymers SAXALEN PPH121GK30 Polypropylene Homopolymer, 30% Glass Filled SAXALEN PPH121GK30 is a 20% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. This type has a higher stiffness and a optimized warpage grade.Informat.. |