Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.00 g/10 min | 1.00 g/10 min | |
S&E Specialty Polymers TufFill™ GPE3003-36 Natural Flame Retardant concentrate in Polyethylene Flame Retardant Concentrate in Polyethylene. GPE3003-36 is PE based, flame retardant concentrate, with 1.47 g/cm3 Gravity and Melt Flow of 1.00, designed to impart flame resistance to polyolefin. De.. |
|||
Melt Flow | 1.00 - 120 g/10 min | 1.00 - 120 g/10 min | Average value: 7.88 g/10 min Grade Count:103 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Melt Flow | 1.00 - 18.0 g/10 min | 1.00 - 18.0 g/10 min | Average value: 6.76 g/10 min Grade Count:44 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Melt Flow | 1.00 - 36.0 g/10 min | 1.00 - 36.0 g/10 min | Average value: 12.2 g/10 min Grade Count:17 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Melt Flow | 1.00 - 64.2 g/10 min | 1.00 - 64.2 g/10 min | Average value: 15.1 g/10 min Grade Count:38 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Melt Flow | 1.00 - 78.7 g/10 min | 1.00 - 78.7 g/10 min | Average value: 32.5 g/10 min Grade Count:22 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Melt Flow | 1.00 - 38.8 g/10 min | 1.00 - 38.8 g/10 min | Average value: 16.8 g/10 min Grade Count:14 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Melt Flow | 1.00 - 55.0 g/10 min | 1.00 - 55.0 g/10 min | Average value: 13.1 g/10 min Grade Count:32 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Melt Flow | 1.00 - 2.00 g/10 min | 1.00 - 2.00 g/10 min | Average value: 1.81 g/10 min Grade Count:10 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Melt Flow | 1.00 - 40.0 g/10 min | 1.00 - 40.0 g/10 min | Average value: 18.4 g/10 min Grade Count:19 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Melt Flow | 1.00 - 53.6 g/10 min | 1.00 - 53.6 g/10 min | Average value: 13.8 g/10 min Grade Count:20 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Melt Flow | 1.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1643L1 Thermoplastic Elastomer Notes: Translucent Features: Tough; Good Melt StrengthInformation Provided by Teknor Apex |
|||
Melt Flow | 1.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1504L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 1.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1580L1-UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 1.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1580-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 1.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1658A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 1.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2322UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 1.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1304 Thermoplastic Elastomer Notes: Translucent Features: Tough; Good Melt StrengthInformation Provided by Teknor Apex |
|||
Melt Flow | 1.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1580L1 Thermoplastic Elastomer Notes: USP Class VI; Translucent Features: High Throughput Uses: Medical TubingInformation Provided by Teknor Apex |
|||
Melt Flow | 1.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1380A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 1.00 - 10.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
1.00 - 10.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB3131 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 1.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1654D Thermoplastic Elastomer Notes: Non-halogenated; RoHS Compliant; MBDC: Green Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General .. |
|||
Melt Flow | 1.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2530F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 1.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Uniprene® UN-2023 Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Flow | 1.00 - 100 g/10 min | 1.00 - 100 g/10 min | Average value: 12.2 g/10 min Grade Count:19 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Melt Flow | 1.00 - 101 g/10 min | 1.00 - 101 g/10 min | Average value: 30.6 g/10 min Grade Count:88 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Melt Flow | 1.00 - 20.0 g/10 min | 1.00 - 20.0 g/10 min | Average value: 10.8 g/10 min Grade Count:9 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Melt Flow | 1.00 - 30.0 g/10 min | 1.00 - 30.0 g/10 min | Average value: 10.1 g/10 min Grade Count:156 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Melt Flow | 1.00 - 280 g/10 min | 1.00 - 280 g/10 min | Average value: 19.3 g/10 min Grade Count:41 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |