Material Notes:
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Melt Flow 1.00 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
1.00 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
ASTM D2240
Tensile Strength at Break 2.93 MPa
425 psi
ASTM D412
Tensile Stress 0.827 MPa
<br>@Strain 100 %
120 psi
<br>@Strain 100 %
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
Tear Strength 10.2 kN/m
58.2 pli
ASTM D624
Compression Set 13 %
<br>@Temperature 22.8 °C,<br> Time 79200 sec
13 %
<br>@Temperature 73.0 °F,<br> Time 22.0 hour
ASTM D395B
24 %
<br>@Temperature 70.0 °C,<br> Time 79200 sec
24 %
<br>@Temperature 158 °F,<br> Time 22.0 hour
ASTM D395B
44 %
<br>@Temperature 100 °C,<br> Time 79200 sec
44 %
<br>@Temperature 212 °F,<br> Time 22.0 hour
ASTM D395B
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746
Processing Properties Metric English Comments
Rear Barrel Temperature 173 - 213 °C
344 - 416 °F
Middle Barrel Temperature 179 - 219 °C
354 - 426 °F
Front Barrel Temperature 184 - 224 °C
364 - 436 °F
Nozzle Temperature 190 - 230 °C
374 - 446 °F
Zone 1 166 - 204 °C
330 - 400 °F
Zone 2 171 - 210 °C
340 - 410 °F
Zone 3 177 - 216 °C
350 - 420 °F
Zone 5 182 - 221 °C
360 - 430 °F
Die Temperature 190 - 227 °C
374 - 440 °F
Melt Temperature 190 - 230 °C
374 - 446 °F
Processing Temperature
Mold Temperature 35.0 - 60.0 °C
95.0 - 140 °F
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Back Pressure 0.172 - 0.862 MPa
25.0 - 125 psi
Cushion 0.381 - 2.54 cm
0.150 - 1.00 in
Screw Speed 50 - 120 rpm
50 - 120 rpm
Descriptive Properties Value Comments
Appearance Opaque