Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Appeel® LSR11N704 Lidding Sealant Resin
(discontinued **) Appeel® 11N704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable seal.. |
|||
Melt Flow | 8.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Appeel® LSR11D704 Lidding Sealant Resin
(discontinued **) Appeel® LSR11D704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable s.. |
|||
Melt Flow | 8.6 g/10 min @Load 6.60 kg, Temperature 295 °C |
8.6 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity... |
|||
Melt Flow | 8.6 g/10 min @Load 6.60 kg, Temperature 295 °C |
8.6 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer (Europe-Africa-Middle East) Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity... |
|||
Melt Flow | 8.6 g/10 min @Load 2.16 kg, Temperature 250 °C |
8.6 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Melt Flow | 8.6 g/10 min @Load 2.16 kg, Temperature 250 °C |
8.6 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Melt Flow | 8.6 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.6 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Melt Flow | 8.6 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.6 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Asia Pacific) Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Melt Flow | 8.6 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.6 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Melt Flow | 8.6 g/10 min @Load 5.00 kg, Temperature 300 °C |
8.6 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Melt Flow | 8.6 g/10 min @Load 2.16 kg, Temperature 235 °C |
8.6 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238R |
UBE PAE1201U Nylon Elastomer Description: UBESTA Nylon 12 ElastomerInformation provided by UBE. |