Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 52 g/10 min @Load 2.16 kg, Temperature 190 °C |
52 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers Kepital® F40-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 52 g/10 min @Load 2.16 kg, Temperature 190 °C |
52 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin Features: High stiffness, high impact strength and low warpage, good top loading capability, high surface gloss.Applications: Container (tub) lids and closures.Data provided by the manufacturer. |
|||
Melt Flow | 52 g/10 min @Load 2.16 kg, Temperature 190 °C |
52 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A; ASTM D1238 |
PolyOne Elastamax™ EG-9065 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun.. |
|||
Melt Flow | 52 g/10 min @Load 10.0 kg, Temperature 220 °C |
52 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AF312 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Melt Flow | 52 g/10 min @Load 10.0 kg, Temperature 220 °C |
52 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AF312T ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Melt Flow | 52 g/10 min | 52 g/10 min | |
Intercontinental Polymers HoPBT 303 HoPBT Polymer Type - Clear, Polyester Pellets Applications: Engineering Resin Information provided by Intercontinental Polymers. |
|||
Melt Flow | 52 g/10 min @Load 5.00 kg, Temperature 260 °C |
52 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® BKV 15 G H2.0 900051 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 15 H2.0, good heat-ageing resistance |
|||
Melt Flow | 52 g/10 min @Load 5.00 kg, Temperature 250 °C |
52 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ420 PBT Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Melt Flow | 52 g/10 min @Load 5.00 kg, Temperature 250 °C |
52 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Melt Flow | 52 g/10 min @Load 5.00 kg, Temperature 250 °C |
52 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Melt Flow | 52 g/10 min @Load 5.00 kg, Temperature 250 °C |
52 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Melt Flow | 52 g/10 min @Load 10.0 kg, Temperature 220 °C |
52 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® NH-1904 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 52 g/10 min @Load 10.0 kg, Temperature 220 °C |
52 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® NH-1904 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 52 g/10 min @Load 5.00 kg, Temperature 250 °C |
52 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ420HP PBT Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Melt Flow | 52 g/10 min @Load 5.00 kg, Temperature 250 °C |
52 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Melt Flow | 52 g/10 min @Load 2.16 kg, Temperature 224 °C |
52 g/10 min @Load 4.76 lb, Temperature 435 °F |
ASTM D1238 |
DSM Biomedical CarboSil® 20 80A Thermoplastic Silicone Polycarbonate Polyurethane (TSPCU) A ground-breaking copolymer that combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic polycarbonate-urethanes Th.. |
|||
Melt Flow | 52 g/10 min @Load 2.16 kg, Temperature 190 °C |
52 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LL 5252.09 Compounding Resin Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending .. |
|||
Melt Flow | 52 g/10 min @Load 2.16 kg, Temperature 190 °C |
52 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 5252.09 Linear Low Density Polyethylene Resin Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending .. |
|||
Melt Flow | 52 g/10 min @Load 2.16 kg, Temperature 250 °C |
52 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
BASF Ultradur B 2550 PBT Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in.. |