Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 32 g/10 min @Load 3.80 kg, Temperature 230 °C |
32 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 41 HF General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
NCMT NanoPAC™ N20 High Performance Polypropylene Nanocomposite Characteristics: Less shrinkage Solved distortion problem Good balance in impact and stiffness High gloss Reduce production cycleApplications: Household Industry Electrical Appliances Toys Industry .. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 190 °C |
32 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers NPP 11-3225 Description: Linear Low Density Polyethylene (LLDP)Information provided by Network Polymers Inc. |
|||
Melt Flow | 32 g/10 min @Load 5.00 kg, Temperature 200 °C |
32 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for.. |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 300 °C |
32 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® BFL2000 PC Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 300 °C |
32 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Asia Pacific) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 300 °C |
32 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylex® P1332L Polycarbonate, UV Stabilized, Unreinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen EP640R Injection Molding Grade Polypropylene Moplen EP640R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640R is a block copolymer particularly suitable for injection.. |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 300 °C |
32 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm |
|||
Melt Flow | 32 g/10 min @Load 3.80 kg, Temperature 230 °C |
32 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CA - 41 HF General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 300 °C |
32 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Europe-Africa-Middle East) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen EP540R Injection Molding Grade Polypropylene Moplen EP540R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540R is a block copolymer particularly suitable for injection.. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 190 °C |
32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Entec Hypel® PEHD32/.951 HDPE
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 190 °C |
32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 2712 HDPE Injection Molding Resin Features: Good stiffness and impact resistance, minimal warpage, good top loading capability, high surface gloss.Applications: Aerosol overcaps, food containers, frozen food containers, seedling tra.. |
|||
Melt Flow | 32 g/10 min @Load 10.0 kg, Temperature 260 °C |
32 g/10 min @Load 22.0 lb, Temperature 500 °F |
ASTM D1238 |
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w.. |
|||
Melt Flow | 32 g/10 min @Load 10.0 kg, Temperature 220 °C |
32 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 32 g/10 min @Load 10.0 kg, Temperature 250 °C |
32 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HI-1001BP PC/ABS, Metal Plating Grade PC/ABS material for platingInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Silon Tabond 5009 Adhesive Resin Tabond 5009 is a chemically modified Polypropylene. This grade is for coextrusion coating of multilayer film to give adhesion between the layers.Characteristics: • Strong adhesion to Aluminium .. |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 224 °C |
32 g/10 min @Load 2.65 lb, Temperature 435 °F |
ASTM D1238 |
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 224 °C |
32 g/10 min @Load 2.65 lb, Temperature 435 °F |
ASTM D1238 |
DSM Biomedical PurSil® 35 Thermoplastic Silicone Polyether Polyurethane (TSPU) A novel copolymer that is strong yet flexible with proven biocompatibility and biostability
Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional.. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil ACHIEVE 3825 Exxpol Metallocene Grade for Nonwovens Fiber and General Extrusion Applications Premium propylene homopolymer resin for fine denier fiber and spunbound applications. Excellent consistency and uniformity for applications involving high speed spinning for fine denier fibers. Con.. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133 |
DSM Arnitel® PL381-H TPC-ET Injection Molding |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 190 °C |
32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a .. |
|||
Melt Flow | 32 g/10 min @Load 10.0 kg, Temperature 220 °C |
32 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Kibisan® PN-107 L125 SAN High Clarity |
|||
Melt Flow | 32 - 37 g/10 min @Load 5.00 kg, Temperature 372 °C |
32 - 37 g/10 min @Load 11.0 lb, Temperature 702 °F |
|
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |
|||
Melt Flow | 32 g/10 min @Load 10.0 kg, Temperature 220 °C |
32 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-11B ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Melt Flow | 32 g/10 min @Load 5.00 kg, Temperature 260 °C |
32 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hybrid B3030 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 32 g/10 min | 32 g/10 min | Condition not noted.; ASTM D1238 |
DuPont Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating 22.5 wt% Vinyl Acetate.Elvax® 3200-2 is an extrudable, wax-modified, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process .. |
|||
Melt Flow | 32 g/10 min @Load 10.0 kg, Temperature 220 °C |
32 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-11B ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 280 °C |
32 g/10 min @Load 4.76 lb, Temperature 536 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Pocan® DP T 7140 LDS 000000 PBT + PET, 44% Mineral + L227Glass Fiber