Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 260 °C |
28 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific) UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 260 °C |
28 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CY6009 PC+ABS (Asia Pacific) CY6009 is a flame retardant (FR) PC+ABS blend with non-brominated and non-chlorinated FR systems. Its excellent flow together with balanced properties and thin wall 5VB capability at less than 2 mm.. |
|||
Melt Flow | 28 g/10 min @Load 1.20 kg, Temperature 300 °C |
28 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP1NREU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains no mold release. |
|||
Melt Flow | 28 g/10 min @Load 1.20 kg, Temperature 300 °C |
28 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 220 °C |
28 g/10 min @Load 22.0 lb, Temperature 428 °F |
JIS K7210 |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 250 °C |
28 g/10 min @Load 11.0 lb, Temperature 482 °F |
cm³/10 min |
Polimeri Europa KOBLEND PCA PD 55 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Halogen free injection moulding grade with flame retardant properties ( UL 94 V-0 at 1.6mm thickness ). Main application fields: business machines, electroni.. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman M3018-P Polyethylene
(discontinued **) Low density polyethylene M3018-P is a specialty formulation suggested for low temperature extrusion coating applications. M3018-P has been found to exhibit good coatability and adhesion to various .. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Iran Petrochemical (PCC) 52528 High Density Polyethylene 52528 is a HDPE copolymer injection molding grade for thin walled applications requiring a good balance between high flowability and physical properties.Application: caps, thin walled, injection mol.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 260 °C |
28 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133-1 |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 260 °C |
28 g/10 min @Load 4.76 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® BF 4130 XF 700051 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, improved flowability |
|||
Melt Flow | 28 g/10 min | 28 g/10 min | ASTM D1238 |
Lucent Polymers PC-1428 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Melt Flow | 28 g/10 min @Load 1.20 kg, Temperature 300 °C |
28 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics PC2800 PC (Europe-Africa-Middle East) PC2800 resin is a high flow (MFR = 28 at 300°C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release... |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 250 °C |
28 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HP-1000XA PC/ABS, Unreinforced PC/ABS material for automobile IP-coreInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 28 g/10 min @Load 3.80 kg, Temperature 260 °C |
28 g/10 min @Load 8.38 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL N750 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business Equipment applications. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 250 °C |
28 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® VB-5305G PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 250 °C |
28 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GN390 PPE+PS (Asia Pacific) Closed loop recycle grade for CANON, 13% PCR-PS loaded, HDT 90C, V-0/1.2mm |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 224 °C |
28 g/10 min @Load 11.0 lb, Temperature 435 °F |
ASTM D1238 |
Lubrizol Pellethane® 2363-75D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3015 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3015 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3015 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3015 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3015 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3015 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3015 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3015 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Melt Flow | 28 g/10 min @Load 8.70 kg, Temperature 224 °C |
28 g/10 min @Load 19.2 lb, Temperature 435 °F |
ASTM D1238 |
Lubrizol Estane® 2355-75A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Memory and elasticity, Impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane pro.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 260 °C |
28 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
Cossa Polimeri ESTABLEND 4501 V0/D Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, PBDE and antimony free, with halogens, high impact resistance, very high thermal resistance, high gloss, good processabilityInformation provided by Cossa Poli.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 265 °C |
28 g/10 min @Load 11.0 lb, Temperature 509 °F |
cm³/10 min. |
Covestro Makroblend® UT-403 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 230 °C |
28 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
ExxonMobil Mytex™ AS33L(W)-06 Talc and rubber modified polypropylene for automotive exterior applications. Offers excellent flow properties and good balance of high stiffness and impact performance.Information provided by ExxonM.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 265 °C |
28 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
Diamond Polymers ABSPC 9802 ABS/PC Molding Grade, High Impact, High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 28 g/10 min @Load 1.20 kg, Temperature 300 °C |
28 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Diamond Polymers PC 2418 R UV UV Stabilized/Mold Release Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 220 °C |
28 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Polylac® PA-763A ABS - Flame Retardant F.R. High Heat |
|||
Melt Flow | 28 - 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
28 - 32 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Breplast Bretene PP Plus Polypropylene Composite Recovered polypropylene compositeInformation provided by Breplast S.p.A. |