Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
PolyOne Trilliant™ HC X THC 1100 Natural Copolyester Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri.. |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 220 °C |
22 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East) Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by .. |
|||
Melt Flow | 22 g/10 min @Load 2.16 kg, Temperature 260 °C |
22 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Asia Pacific) Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Melt Flow | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Melt Flow | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP2REU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a h.. |
|||
Melt Flow | 22 g/10 min @Load 0.325 kg, Temperature 270 °C |
22 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVALEN PH 91 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Melt Flow | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Melt Flow | 22 - 32 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 - 32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 220 °C |
22 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical HI121U ABS Feature: Injection Molding, Well Balanced Mechanical Properties, Good weatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemic.. |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 220 °C |
22 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
Ineos ABS Lustran® LGA Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Melt Flow | 22 g/10 min @Load 2.16 kg, Temperature 230 °C |
22 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 2-2120 17TOP BU UV-Stabilized 17% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-2120 17TOP BU is a black colored, 17% talc-filled, UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-2120 17TOP BU is developed for producing injection .. |
|||
Melt Flow | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics PC2203R PC (Europe-Africa-Middle East) PC2203R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 220 °C |
22 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Novodur® P2M-AT ABS Pellets Novodur® P2M-AT has high impact strength, high gloss, and contains antistatic additive. It is used for the production of molded plastic articles. |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 250 °C |
22 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HP-1000P PC/ABS, Unreinforced High flow material that can be used in the exterior material of mobile phone, wheel cap, rice cooker, electric iron etc. as well as refrigerator door handle and panelInformation provided by Samsung .. |
|||
Melt Flow | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Samyang Trirex® PC-3020HF 22 MFI Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Samyang Trirex® PC-3020U 22 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 250 °C |
22 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HP-1000P PC/ABS, Unreinforced High flow material that can be used in the exterior material of mobile phone, wheel cap, rice cooker, electric iron etc. as well as refrigerator door handle and panelInformation provided by Samsung .. |
|||
Melt Flow | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Yellow 2057E Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2057E is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2057E is h.. |
|||
Melt Flow | 22 g/10 min | 22 g/10 min | ISO 1133 |
Tisan TISARBON® UNR Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 220 °C |
22 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Polyram RamShine PV701 ABS, UV Stabilized UV stabilized ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melt Flow | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Wonderlite® PC-122U Polycarbonate - UV Stabilized UV Stabilized |
|||
Melt Flow | 22 g/10 min @Load 3.80 kg, Temperature 230 °C |
22 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Dow Retain® 8209 ABS + Polycarbonate Data provided by Dow Chemical. |
|||
Melt Flow | 22 - 28 g/10 min @Load 3.80 kg, Temperature 230 °C |
22 - 28 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Melt Flow | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Barlog Plastics KEBAFORM C 8027 POM Copolymer, 30% mineral reinforced POM-MD30Information provided by BARLOG plastics GmbH. |
|||
Melt Flow | 22 g/10 min @Load 2.16 kg, Temperature 250 °C |
22 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
BASF Ultradur B 4300 G3 15% Glass Filled PBT Ultradur B 4300 G3 is an easy flowing injection molding PBT with 15% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Melt Flow | 22 g/10 min @Load 2.16 kg, Temperature 230 °C |
22 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem CP 204 Injection Molding Polypropylene Description: CP 204 is a high melt flow rate heterophasic copolymer with general purpose additive package. This product exhibits excellent processing performance, with good stiffness and impact stre.. |