Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT4900-74UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 17 g/10 min | 17 g/10 min | ASTM D1238 |
Mytex Polymers AS23K-01 Polypropylene, Talc filled, Compounded, Non-UV stabilized Description: A non-UV stabilized talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation pro.. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® LUX2289 PC Lexan* LUX2289 resin is an injection molding grade with high light reflectance |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East) Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 190 °C |
17 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 2710 HDPE Injection Molding Resin Features: Good ESCR, good processability.Applications: Housewares, containers, toys.Data provided by the manufacturer. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 343 °C |
17 g/10 min @Load 4.76 lb, Temperature 649 °F |
ASTM D1238 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)
(Unverified Data**) Udel P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel P-1700 and a slightly greater t.. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 260 °C |
17 g/10 min @Load 4.76 lb, Temperature 500 °F |
ISO 1133-1 |
Lanxess Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Melt Flow | 17 - 27 g/10 min | 17 - 27 g/10 min | ASTM D1238 |
Lushan EV1050G1 EVA Film for Encapsulating Solar modules, Ultra Fast Cure EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemica.. |
|||
Melt Flow | 17 - 27 g/10 min | 17 - 27 g/10 min | ASTM D1238 |
Lushan EV1050G1/RF EVA Film for Encapsulating Solar modules, Reinforced Friendly EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemica.. |
|||
Melt Flow | 17 - 19 g/10 min @Load 5.00 kg, Temperature 200 °C |
17 - 19 g/10 min @Load 11.0 lb, Temperature 392 °F |
Granulate; ISO 1133/H |
SYNTHOS Krasten® 137 General Purpose Polystyrene Easy flow. Examples of Application:Injection moulding – cups and containers for the food industry, medical devices, drawing templates.Extrusion – coextrusion, high gloss surface.Synthos wa.. |
|||
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 200 °C |
17 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution PS 153A GPPS Styrolution PS 153A is an antistatic modified, general purpose polystyrene grade with a good flow characteristic.AntistaticGood flow characteristicsInformation provided by Styrolution |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 270 °C |
17 g/10 min @Load 2.65 lb, Temperature 518 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific) This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 17 g/10 min @Load 10.0 kg, Temperature 220 °C |
17 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SR-0305 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 260 °C |
17 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
Cossa Polimeri ESTABLEND PSA 7800 PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
estimated from MVR using room temperature density; ISO 1133 |
Covestro Makrolon® 2558 Polycarbonate ISO 7391-PC,MR,(,,)-18-9MVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for ETO and steam sterilization at 121 °CComplies with the requirements of FDA-modified ISO 10993-1 and USP Class.. |
|||
Melt Flow | 17 g/10 min | 17 g/10 min | ASTM D1238 |
ExxonMobil Exact™ 3040 Cast Ethylene-based Plastomer Resin Product Description: Exact 3040 is an ethylene-based hexane copolymer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3040 is designed for monolayer and coextrusion cast fi.. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Entec Hylex® P1017FR Polycarbonate Information provided by Ravago. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil PP7654KNE2 Polypropylene Homopolymer Product Description: A high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded large consumer and industrial parts.Availabili.. |
|||
Melt Flow | 17 g/10 min | 17 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Copolymer CP0437W30L Wollastonite Reinforced |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 280 °C |
17 g/10 min @Load 4.76 lb, Temperature 536 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET) 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol.. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ PB4432 TPO Compound Daplen PE4432 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen PE4432 is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Melt Flow | 17 g/10 min @Load 10.0 kg, Temperature 220 °C |
17 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min |
Polimeri Europa SINKRAL PD G120 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-09-30 General purpose injection moulding grade. Characteristics: outstanding rigidity very high surface.. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Hifax™ HSBMF248 Thermoplastic Polyolefin Elastomer Description: Hifax™ HSBMF248 high melt flow, 1,400 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of flow, rigidity, low t.. |