Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10 g/10 min @Load 0.325 kg, Temperature 270 °C |
10 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVALEN PH 66 GF 20 FRO 4 PP, 20% glass fibre, flame retardant FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre, with decreased flammability. Used in the electrical industry - teroderately increased toughness an.. |
|||
Melt Flow | 10 g/10 min @Load 0.325 kg, Temperature 270 °C |
10 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVALEN PH 72 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, thermo stable, chemically modified talc. General application in all industry branches - covers of.. |
|||
Melt Flow | 10 g/10 min @Load 0.325 kg, Temperature 270 °C |
10 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVALEN PQ 81 T 30 PP, 30% mineral filling FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Melt Flow | 10 g/10 min @Load 0.325 kg, Temperature 270 °C |
10 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVAMID 6 FRM 2 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 230 °C |
10 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
NCMT NanoPAC™ G2050H High Performance Polypropylene Nanocomposite Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 230 °C |
10 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers NPP 25-1010 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 943X PC Copolymer Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Melt Flow | 10 g/10 min @Load 10.0 kg, Temperature 240 °C |
10 g/10 min @Load 22.0 lb, Temperature 464 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 TPC-ET
(Unverified Data**) Hytrel® HTR8441 is a 55 nom. Shore D thermoplastic polyester elastomer for blow molding. It provides good mechanical properties at high temperature.Information provided by DuPont Performance Polyme.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 945U PC Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Melt Flow | 10 g/10 min @Load 5.00 kg, Temperature 200 °C |
10 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Nova 765 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, High impact, Color stable, Custom colorsApplications: High flow, multi-purpose injection molding grade where color stability is a requirement, Toys, Appliance, Computer peripheralsPerform.. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | |
Microcell Composite Company CELLIFF® 7000 Polymer Pellets CELLIFF® special high polymer materials are mixed for high degrees of hardness and tenacity. For producing stiff, light weight foaming boards which are tenacious and durable. The foam surface can.. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 E |
Micropol Microcoat DG/EVA/214A Microground modified EVA copolymer Specially developed for high specification coating where metal/coating adhesion is of primary importance. Typically used on large flat surfaces, and when toughness, elasticity and excellent barrier .. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
LTL Color Compounds ColorFast® PC100 Polycarbonate 10 melt standard injection molding gradeAll information provided by LTL Color Compounders, Inc. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Styron EMERGEâ„¢ 8600-10 Polycarbonate EMERGEâ„¢ PC 8600-10 is a translucent, ignition-resistant polycarbonate resin. The resin contains no bromine, chlorine or phosphate additives and is intended to comply with global environmental .. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Polyram RamTough PZ333G2 Polycarbonate, 10% Glass Fiber, Flame Retardant 10% glass fiber reinforced, flame retardant polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238L |
Total PPR 7525MZ Polypropylene, Injection Molding Grade Clarified random copolymer for injection moldingClarity - FINA 7525MZ exhibits superior clarity in molded parts.Impact - FINA 7525MZ produces molded parts with improved impact compared with parts mo.. |
|||
Melt Flow | 10 g/10 min @Load 5.00 kg, Temperature 200 °C |
10 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total PS CPDS 818E Flame Retardant Polystyrene POLYSTYRENE (PS) COMPOUND (CPDS) 818E is a high impact brominated flame retardant polystyrene. A combination of high flow and high heat stability gives excellent processability and reduced cycle ti.. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
A. Schulman POLYFLAM™ FPP 1007F Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007F is a 40% talc filled homopolymer polypropylene compound that utilizes FDA compliant raw materials.Information provided by A. Schulman. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 10 g/10 min @Load 5.00 kg, Temperature 190 °C |
10 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
ELASTO UK Dryflex® 602500S SEBS Based Material, Filled Qualities, 50A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 2805 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Wonderlite® PC-110V Polycarbonate - Flame Retardant |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 230 °C |
10 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil AP3AW Polypropylene Impact Copolymer Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe.. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg |
10 g/10 min @Load 4.76 lb |
|
Dow HDPE 10462N High Density Polyethylene DOW HDPE 10462N resin is a narrow molecular weight distribution polymer designed to offer good stress crack resistance and impact strength with excellent rigidity. This resin has good processability.. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
A. Schulman POLYFLAM™ FPP 1006S Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006S is a 20% talc filled homopolymer polypropylene compound formulated with an internal mold release. Information provided by A. Schulman. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | melt index; ASTM D1238 |
Asahi Kasei Tenac®-C EF750 Acetal Copolymer, Antistat
(discontinued **) Antistatic grade containing special carbon black.Applications: Parts requiring antistatic properties.This product is not a part of the standard product line dated 2003. |
|||
Melt Flow | 10 - 15 g/10 min @Load 5.00 kg, Temperature 190 °C |
10 - 15 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polyplastic Armoflen® PO MF 75-1 Polypropylene Homopolymer, 75% Calcium Carbonate Information provided by PolyPlastic Group. |