Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.0 - 15 g/10 min | 8.0 - 15 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 6821 C BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 8.0 - 15 g/10 min | 8.0 - 15 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE D 4210 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 10 - 15 g/10 min @Load 2.16 kg, Temperature 230 °C |
10 - 15 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 8300N Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 2.16 kg, Temperature 265 °C |
5.0 - 15 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Melt Flow | 8.0 - 15 g/10 min | 8.0 - 15 g/10 min | ASTM D1238 |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 2.16 kg, Temperature 250 °C |
5.0 - 15 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Melt Flow | 10 - 15 g/10 min @Load 2.16 kg, Temperature 250 °C |
10 - 15 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-M30 Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced Warpage Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 2.16 kg, Temperature 265 °C |
5.0 - 15 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
Polymer Resources PC/TP-GP1 PC/Polyester Alloy High Impact, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Pol.. |
|||
Melt Flow | 10 - 15 g/10 min | 10 - 15 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 10 - 15 g/10 min | 10 - 15 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 2.16 kg, Temperature 150 °C |
5.0 - 15 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-620 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 2.16 kg, Temperature 150 °C |
5.0 - 15 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-640 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 2.16 kg, Temperature 150 °C |
5.0 - 15 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-650 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 2.16 kg, Temperature 150 °C |
5.0 - 15 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-810 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized... |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 2.16 kg, Temperature 150 °C |
5.0 - 15 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-853 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 2.16 kg, Temperature 150 °C |
5.0 - 15 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-530 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 10 - 15 g/10 min | 10 - 15 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |
|||
Melt Flow | 8.0 - 15 g/10 min | 8.0 - 15 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Melt Flow | 8.0 - 15 g/10 min | 8.0 - 15 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Melt Flow | 8.0 - 15 g/10 min | 8.0 - 15 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 8.70 kg, Temperature 175 °C |
5.0 - 15 g/10 min @Load 19.2 lb, Temperature 347 °F |
|
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Melt Flow | 12 - 15 g/10 min | 12 - 15 g/10 min | ISO 1133 |
Chengdu Polyster H6055 Thermoplastic Polyether-ester Elastomer (TPEE) Medium modulus molding and injection grade. Contains improved color- stable antioxidants. Higher melt flow index compared with other grades; good balance of modulus and toughness. Applications requi.. |
|||
Melt Flow | 10 - 15 g/10 min @Load 5.00 kg, Temperature 372 °C |
10 - 15 g/10 min @Load 11.0 lb, Temperature 702 °F |
|
Daikin NEOFLON AP-210AS PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D.. |
|||
Melt Flow | 12 - 15 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 - 15 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
AKG Polymers Vision PP PPH BL1302 T20 Polypropylene Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Melt Flow | 1.0 - 15 g/10 min @Load 3.80 kg, Temperature 232 °C |
1.0 - 15 g/10 min @Load 8.38 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st.. |
|||
Melt Flow | 10 - 15 g/10 min | 10 - 15 g/10 min | ISO 1133 |
Beijing Ranger Chem BLUESTAR® 1120 PBT Can be used directly to produce cable sheathInformation provided by Beijing Ranger Chemical Co. |
|||
Melt Flow | 8.0 - 15 g/10 min | 8.0 - 15 g/10 min | ASTM D1238 |
Buckeye Polymers BP RPP 3009 GK BLK Polypropylene, Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |
|||
Melt Flow | 8.0 - 15 g/10 min | 8.0 - 15 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Melt Flow | 6.0 - 15 g/10 min | 6.0 - 15 g/10 min | ASTM D1238 |
Buckeye Polymers BP RPP 2012 T NAT Polypropylene, Calcium Carbonate Filled Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges fro.. |