Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm

@Thickness 6.35 mm
0.0030 - 0.0040 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® J-68/20/E/SD/HM Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled, with static dissipation
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm

@Thickness 1.60 mm
0.0010 - 0.0040 in/in

@Thickness 0.0630 in
horizontal; ASTM D955
Gromax PBT 5130-104 30% Glass Fiber Filled
CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion..
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm

@Thickness 6.35 mm
0.0030 - 0.0040 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® J-61/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm

@Thickness 6.35 mm
0.0030 - 0.0040 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® J-62/30/E8 Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm

@Thickness 6.35 mm
0.0030 - 0.0040 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® J-68/20/E/SD Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled, with static dissipation
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.0025 - 0.0040 cm/cm

@Thickness 6.35 mm
0.0025 - 0.0040 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® J-68/25/E/SD Polypropylene Copolymer, 25% Glass Fiber Reinforced, Chemically coupled, with static dissipation
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 80°C; ASTM D955
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 80°C; ASTM D955
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 1.00 mm
0.0020 - 0.0040 in/in

@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® T-402 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 1.00 mm
0.0020 - 0.0040 in/in

@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® T-521 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 1.00 mm
0.0020 - 0.0040 in/in

@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 1.00 mm
0.0020 - 0.0040 in/in

@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® T-663G50A MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 1.00 mm
0.0020 - 0.0040 in/in

@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® T-669VGB Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 1.00 mm
0.0020 - 0.0040 in/in

@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 80°C; ASTM D955
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 80°C; ASTM D955
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 80°C; ASTM D955
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm

@Thickness 6.35 mm
0.0030 - 0.0040 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® J-62/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 1.60 mm
0.0020 - 0.0040 in/in

@Thickness 0.0630 in
horizontal; ASTM D955
Gromax CCP PBT 3040-201 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
48 hr at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm

@Thickness 6.35 mm
0.0030 - 0.0040 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® J-68/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics