Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0010 cm/cm @Thickness 1.60 mm |
0.0010 in/in @Thickness 0.0630 in |
Flow; DAM |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm @Thickness 3.17 mm |
0.0010 - 0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-68/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 1.60 mm |
0.0010 - 0.0030 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP PET 9130-104 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm @Thickness 1.60 mm |
0.0010 - 0.0040 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP ABS/PBT 7320H-104 20% Glass Fiber Filled Product Description: A 20% glass fiber reinforced injection molding grade. Characteristics:Low warp age and excellent dimensionally stable Excellent electrical property Excellent mechanic and chemi.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm @Thickness 1.00 mm |
0.0010 - 0.0020 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
48 hr, at 80 and 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
48 hr, at 80 and 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |