Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
PolyOne Trilliant™ HC HC6620-0033 RS Natural Polyamide 66 (Nylon 66) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 - 0.019 cm/cm | 0.017 - 0.019 in/in | ASTM D955 |
PolyOne Stat-Tech™ NN-20CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4, 2577 |
Kuraray Genestarâ„¢ N1001D-U83/02 Nylon Standard unreinforced extrusion grade. Main Features:Outstanding fuel barrierHeat resistanceExample of applications:Multi-layered fuel tube |
|||
Linear Mold Shrinkage, Transverse | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | |
LATI Latiohm 75/4-10 CNT PBT Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | |
LATI Latishield 75/4-10A PBT, Steel Fiber Reinforced EMI shielding product based on Polybutylene Terephthalate (PBT). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 - 0.019 cm/cm @Thickness 3.18 mm |
0.017 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 - 0.020 cm/cm @Time 86400 sec |
0.017 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
Teknor Apex Telcar® TL-1522E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® 2D 20 nat PA612 Product Description: Grilamid 2D 20 natural is an unmodified unreinforced, medium viscosity polyamide 612 (PA612), designed for injection molding as well as extrusion. It is characterized by the fol.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® 2S 25 W 20 X nat PA610-I Product Description: GRILAMID 2S 25 W 20 X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified polyamide 610, especially suitable for extrusion applications. This PA610.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100TL NC010 (formerly Delrin 100TL NC000) is a high viscosity acetal homopolymer with 1.5% TeflonInformatio.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 911DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear .. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | Eurotec |
Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, improved impact, heat stabilized, black Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
Clariant PA233 Nylon 6, Improved Processability, Easily Colorable, Toughened Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | |
Eurotec® Tecomid® NA40 NL IH PA 6.6 impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 |
Barlog Plastics KEBATER BM330 PBT, 30% mineral reinforced, good light reflection PBT-MD30Information provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, Conditioned Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL is a high viscosity acetal homopolymer, containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.Inform.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | 60x60x2mm; ISO 294 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | MPC method |
Mitsui TPX® MX004 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | MPC method |
Mitsui TPX® RT18 XB Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | Sheet |
BASF Ultradur B 6550 L PBT Ultradur B 6550 L is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |