Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ASTM D955 |
Multibase Multi-Flex® TPE A 6821 NAT This product is based on Kraton G and PP. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | STN EN ISO 294-4 |
Plastcom SLOVAMID® 6 NG1 GF 30 HLS PA6 reinforced with glass fiber, UV stabilized, hydrolysis resistant PA 6 for injection molding, reinforced with 30% glass fiber, for moldings used in the automotive, weather and UV stabilized. Determined for using in outside automotive applications like door handle,.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ASTM D955 |
PolyOne Trilliant™ HC HC9820-0030 RS Natural Polyetheretherketone (PEEK) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 2.00 mm |
0.011 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® SK612SF NC010 PBT
(Unverified Data**) Crastin® SK612SF is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | LATI |
LATI LARPEEK 10 K/20 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 2.00 mm |
0.011 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66
(Unverified Data**) Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 |
DSM Akulon® K223-KM6 Nylon 6-30% Mineral Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | 60x60x2; 270°C / WZ 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66 PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | 60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Pocan® BF 4232 HR 901510 PBT, 30% Glass Fiber PBT, 30% glass fiber, injection molding, flame retardant, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | |
Solvay TECHNYL® A 50H1 PA66, DRY Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.012 cm/cm | 0.011 - 0.012 in/in | mold temp=100°C; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm @Time 86400 sec |
0.011 - 0.013 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07435 LNP* THERMOCOMP* is a compound based on Miscellaneous resin containing Proprietary Filler(s). Added feature of this grade is: Plateable. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp WC003P Polyester Elastomer LNP* Thermocomp* WC003P is a compound based on Polyester resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Sim. To ISO 294-4 |
DSM Akulon® CO-KGV4 /A JN.00.86 PA6-GF20 FR % Glass Reinforced, Heat Stabilized, Flame Retardant (halogen-phosphorous-free) |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Sim. To ISO 294-4 |
DSM Novamid® 1010C2 PA6 Easy Molding Grade |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® AS V0 PA66 Product description: Grilon AS V0 is an unreinforced, normal viscosity, self-extinguishing PA66 injection molding grade. Grilon AS V0 has the following important properties: Halogen and phosphorous-.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | |
E-Polymers TEKAFIN® PH70G1 HIPP + 10% Glass Fiber Reinforced Scratch Resistance Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Eurotec |
Eurotec® Tecodur® PB70 GR30 NL100 PBT, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Eurotec |
Eurotec® Tecomid® NA40 CR10 BK111 PA6.6, 10% carbon fiber reinforced, black Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Eurotec |
Eurotec® Tecomid® NB40 GR15 NL HS PA6, 15% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.011 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 GF30 TF15 Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO Data (Dry) |
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® SK695FR BK507 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |