Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | 380°C nozzle, 190°C tool; ISO 294-4 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Thickness 2.00 mm |
0.0090 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® 74G33W NC010 Nylon 66
(Unverified Data**) Zytel® 74G33W NC010 is a 33% glass reinforced nylon 66 and nylon 6 co-melt resin with improved weatherability.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4, 2577 |
Kuraray Genestarâ„¢ G1350A-M42 Nylon, 35% Glass Filled 35% Glass reinforced injection grade. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment.Main Features:Hydrolysis resistanceHeat resista.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Thickness 2.00 mm |
0.0090 in/in @Thickness 0.0787 in |
ASTM D955 |
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant Vypet VNT 615 FR is a 15% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | Dry; ASTM D955 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.019 cm/cm | 0.0090 - 0.019 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | |
Toyobo ECOVYLOPET® EMC2311 PET Bottle Recycling Grade, 10% Glass Reinforced Features: PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | |
Toyobo Vylopet® EMC130-01 Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric stren.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | |
Toyobo VYLOPET® EMC532 Injection Molding Polyester Resin, Glass Reinforced Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | DAM; ISO 294-4 |
DSM Akulon® K224-G6U (Cond.) 33% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | Sim. To ISO 294-4 |
DSM Arnite® AV2 370 XL-T PET-GF35 35% Glass Reinforced, Low Outgassing, Thermal conductive material |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Thickness 4.00 mm |
0.0090 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600 CF10 HWCP 10% Carbon Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® XE 4106 nat PA612-GF30 Product description: Grilamid XE 4106 natural is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorptiong.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® CE15330 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Thickness 2.00 mm |
0.0090 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | |
Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | |
E-Polymers TEKASTER® F10G30FR 30% Glass Fiber Reinforced Flame Retardant PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | Eurotec |
Eurotec® Tecopet® PT74 GR30 NL XA60 PET, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free,, heat stabilized, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4 |
Barlog Plastics KEBAFLEX SG 85 A.1 TPE-S, Shore A85, natural TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Diameter 2.00 mm |
0.0090 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4 |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Conditioned, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4 |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | |
E-Polymers SEPAZ® N5020HI Nanoclay 4%, 30% Glass Fiber Reinforced High Impact Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | Eurotec |
Eurotec® Tecomid® NB40 NL FN70 PA6, unfilled, flame retardant - halogen free (RoHS compliant), natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4, 2577 |
Lanxess Durethan® BM 25 FN20 DUS013 000000 Nylon 6, 25% Mineral PA 6, injection molding grade, 25% mineral, UL94V-2 off 0.75 mm, max. temp. glow wire test:960°C off 0.8 mm, free from halogen, optimized for laser marking at 1064 nm, |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4, 2577 |
Kuraray Genestar™ G1300A-M41 Nylon, 30% Glass Filled Glass reinforced injection grade. Main Features:Chemical resistanceHeat resistanceExamples of applications:Gears and bearing retainersIntercooler tank and turbo duct pipe |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East) VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | 380°C nozzle, 180°C tool; ISO 294-4 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |