S&E Specialty Polymers GA-2285FR PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GA-2285FR PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: 80°C clear flame retardant PVC compound.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.26 - 1.32 g/cc
1.26 - 1.32 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 90
85 - 90
ASTM D2240
Tensile Strength 12.8 MPa
1860 psi
ASTM D412
Elongation at Break 340 %
340 %
ASTM D412
Thermal Properties Metric English Comments
Oxygen Index 26 %
26 %
ASTM D2863