Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
ASTM D792
S&E Specialty Polymers TufTech™ GA-1050-02LF PVC Compound
Application: A 105°C, AWM, 90°C AWM 1,000 volt, flame retardant compound.Information provided by S&E Specialty Polymers
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
Dow BETADAMP™ 32HT  (discontinued **)
BETADAMP™ 32HT is a high temperature vibration damper that can be applied to the exterior of cast aluminum or steel engine valve, transmission, and crankcase (oil pan) covers or electro-coat substr..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
NBR NM-IEC 60811-1-3
Karina E810-40/312-IS-RG Green PVC Compound
Non toxic PVC compound, recommended for blow molding of bottles for alcoholic beverages.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
NBR NM-IEC 60811-1-3
Karina 36/234-FC-LMP (SDB) Brown Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D 792
Karina 970-DA-48/1-B-IS Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
ASTM D 792
Karina E 18/35-FC-LMP Gray Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
ASTM D 792
Karina E 74/240-D-IS-SD-TR Compound PVC Crystal
Films laminated shrinkInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 8571 Moldings & Extrusions Flexible PVC
High quality, semi-rigid extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required.Information provided by Georgia GulfGeorgia ..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 12770 Coax & Telecom Flexible PVC
Non-lead stabilized, CATV and general purpose jacket with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 15642 Wire & Cable Flexible PVC
Non-lead stabilized semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 15643 Wire & Cable Flexible PVC
Non-lead stabilized semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C. The compound is also formulated for fungus and microbe resistanc..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 16860 Wire & Cable Flexible PVC
Battery booster jacket compound and general purpose jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 18730 Wire & Cable Flexible PVC
UL recognized 720 hour sunlight resistant in all colors, oil resistant, 105 C rated PVC jacket compound with good low temperature performance. Information provided by Georgia GulfGeorgia Gulf became..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 19450 Wire & Cable Flexible PVC
105°C rated insulation compound with very good migration and oil resistance. Recommended for toner resistant applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 312 Wire & Cable Flexible PVC
General purpose jacketing and insulation compound. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 38552 Wire & Cable Flexible PVC
General purpose insulating and jacketing compound for 105°C AWM and SPT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 38702 Moldings & Extrusions Flexible PVC
Flame retardant CATV and general purpose jacket with excellent low temperature properties. UL approved for 720 hour sunlight resistance in all colors. UL approved for 94 V-0 at 1.5 mm in all color..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 8552 Moldings & Extrusions Flexible PVC
A soft extrusion compound recommended for profiles, weatherstrips and sheeting. Also suitable for injection molding.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 11441 Wire & Cable Flexible PVC
Clear extrusion compound formulated for applications necessitating a high degree of flame retardancy.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 18731 Wire & Cable Flexible PVC
Non-lead stabilized, UL recognized 720 hour sunlight resistant in all colors, 105 C rated jacket compound with good low temperature performance.Information provided by Georgia GulfGeorgia Gulf becam..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 19470 Wire & Cable Flexible PVC
Semi-rigid, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by Georgia ..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 19481 Wire & Cable Flexible PVC
105°C, VW-1 rated non-lead stabilized insulation. Best suited for small gauge, 1/64 wall applications. UL approved for TW, THW, THHW, THHN-THWN insulation.Information provided by Georgia GulfGeor..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 19482 Wire & Cable Flexible PVC
105°C, VW-1 rated non-lead stabilized insulation compound. Ideally suited for 18 AWG, 1/64 wall. UL approved for TW, THW, THHW applications.Information provided by Georgia GulfGeorgia Gulf became..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 19805 Wire & Cable Flexible PVC
Non-lead stabilized primary insulation and jacketing compound recommended for 105°C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 19854 Wire & Cable Flexible PVC
Non-lead stabilized, 105°C rated insulation compound. Recognized by UL for TW and THW applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 10702 Wire & Cable Flexible PVC
General purpose 80°C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 19471 Wire & Cable Flexible PVC
Semi-rigid, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by Georgia ..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 4441 Flexible PVC
85C non-lead stabilized wire harness. SAE J1128.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 286FR Moldings & Extrusions Flexible PVC
105C plug molding compound. UL recognized component for 94 V-2 in all colors (0.75 mm min. thickness). UL QMFZ2 recognized component.Information provided by Georgia GulfGeorgia Gulf became Axiall ..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 8918 Moldings & Extrusions Flexible PVC
Non-lead migration resistant extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.